HumiSeal 1A33LOS is a high-performance, single-component polyurethane coating that eliminates the safety risks associated with traditional isocyanates. Ideal for high-reliability PCBs, it provides a tough, chemical-resistant shield while remaining low-odor and low-toxicity. With UV fluorescence for inspection and full RoHS compliance, it offers a "no-compromise" transition from standard 1A33 to a safer, more sustainable production process.

Product Key Features

  • Single-component polyurethane conformal coating
  • Reduced odor formulation with lower toxicity solvents
  • Comparable cured performance to HumiSeal 1A33
  • Fluoresces under UV light for easy inspection
  • No free isocyanates
  • Low moisture vapor permeability
  • Available in ready-to-use pre-blended viscosities
  • RoHS Directive 2015/863/EU and China RoHS 2 compliant

Applications

  • Printed circuit board (PCB) protection
  • Consumer electronics assemblies
  • Industrial electronics
  • Telecommunications equipment
  • Automotive electronic modules
  • Power supply assemblies
  • Electronic assemblies requiring low-odor coatings
Product Family

HUMISEAL 1A33LOS

1. Select Package Size

Loading pricing…

Product availability
EU Shipping in 6 weeks
Packaging
Please select Package Size.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Density (g) Density (g)
0.92 g/cm3
Film Thickness Film Thickness
25 - 75 µm
Solids Solids
44 %
Physical Properties
Viscosity Viscosity
195 mPa.s
Thermal Properties
Glass Transition Temperature (Tg) Glass Transition Temperature (Tg)
26 °C
Operating Temperature Operating Temperature
-65 - 125 °C

Additional Information

Learn More About HumiSeal® 1A33LOS

Application Methods

HumiSeal® 1A33LOS is available in pre-blended viscosities for immediate use, supporting multiple application techniques.

  • Dipping: Apply using a controlled immersion and withdrawal rate of 5–15 cm/min to ensure uniform coating thickness. Monitor viscosity regularly and adjust with approved thinner as needed.

  • Spraying: Pre-blended grades can be sprayed using conventional spray equipment. Adequate ventilation is required to remove solvent vapors and mist.

  • Brushing: Suitable pre-blends may be applied by brush. Film uniformity depends on viscosity selection and operator technique.

Important Notes:

  • Substrate cleanliness is critical for coating performance.
  • Perform compatibility testing prior to production use.
  • Consult HumiSeal® Technical Support for pre-blend selection.

Application Compatibility

HumiSeal® 1A33LOS is compatible with a wide range of materials used in electronic assemblies.

Compatible With:
✔ FR-4 and common PCB substrates
✔ Metals and plated finishes
✔ Most electronic components
✔ Automated coating equipment

Not Recommended For:
✖ Contaminated or moisture-laden substrates
✖ Application near open flames or ignition sources

Additional Guidance:
Always verify material compatibility and cleanliness prior to coating. UV fluorescence allows easy inspection and repair after application.


Safety and Handling Precautions ⚠️

  • Use only in well-ventilated areas
  • Avoid inhalation of vapors or spray mist
  • Avoid contact with skin and eyes
  • Keep away from sparks, heat, and open flames
  • Follow local and national health and safety regulations

Always consult the Safety Data Sheet (SDS) before use.

Storage Recommendations 📦

Store HumiSeal® 1A33LOS and its pre-blends in tightly closed containers away from excessive heat or cold. Recommended storage temperature is 0–35°C. Allow material to equilibrate for 24 hours at 18–32°C before use.


Compliance You Can Trust ✅

HumiSeal® 1A33LOS meets international reliability and compliance standards:

✔ RoHS Directive 2015/863/EU compliant
✔ China RoHS 2 compliant
✔ No free isocyanates
✔ UV fluorescent for inspection and quality control