Main features

  • Single-component polyurethane conformal coating
  • UL 94 V-0 Flame Retardant
  • No free isocyanates

Product Description

HumiSeal 1A27 LTX is a high-performance, single-component polyurethane conformal coating designed for advanced PCB protection. Engineered with a low-VOC formulation, it meets stringent environmental regulations—including China’s GB30981-2020—without compromising on performance.

Product Key Features

  • Single-component polyurethane conformal coating
  • Protection against moisture, corrosive environments, and contamination
  • Low moisture vapor permeability for long-term reliability
  • Easy application using automated or manual methods
  • Reduced xylene and toluene formulation
  • No free isocyanates
  • Compliant with GB30981-2020 VOC regulations
  • UL 94 V-0 flame retardant

Applications

  • General printed circuit board (PCB) protection
  • Consumer, industrial, and automotive electronics
  • Assemblies exposed to moisture, dust, or corrosive environments
  • Electronics requiring long-term insulation resistance and dielectric strength
Product Family

HUMISEAL 1A27LTX

1. Select Package Size

Loading pricing…

Product availability
EU Shipping in 6 weeks
Packaging
Please select Package Size.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Solids Solids
50 %
Thickness range Thickness range
0.025 - 0.075 mm
Physical Properties
Viscosity Viscosity
3000 mPa.s
Thermal Properties
Glass Transition Temperature (Tg) Glass Transition Temperature (Tg)
28 °C
Electrical Properties
Breakdown Voltage Breakdown Voltage
7500 V

Additional Information

Learn More About HumiSeal® 1A27 LTX

Application Methods

HumiSeal® 1A27 LTX is designed for flexible application across automated and manual coating processes.

Application Methods:

  • Dipping: Viscosity may be adjusted using HumiSeal® Thinner 789 to ensure uniform film thickness. Controlled immersion and withdrawal rates of 5–15 cm/min are recommended. Viscosity should be monitored regularly using Zahn or Ford cups.
  • Spraying: Suitable for conventional spray equipment. Thinning with HumiSeal® Thinner 789 is required to achieve a uniform, pinhole-free coating. Adequate ventilation must be provided.
  • Brushing: Can be applied by brush with minor thinning. Final film quality depends on component density and operator technique.

Important Notes:

  • Substrates must be clean, dry, and free of flux, grease, and contaminants.
  • Contamination beneath the coating can lead to electrical or mechanical failure.
  • Allow sufficient curing time to reach optimum performance.

Application Compatibility

HumiSeal® 1A27 LTX is compatible with a wide range of PCB materials and electronic components.

Compatible With:
✔ Printed circuit boards and electronic assemblies
✔ Automated dip, spray, and selective coating systems
✔ Standard electronics manufacturing materials

Additional Guidance:
For optimal performance, ensure proper cleaning prior to coating. Consult Technical Support for guidance on viscosity adjustment, equipment selection, or pre-blend solutions.


Safety and Handling Precautions ⚠️

  • Use only in well-ventilated areas.
  • Avoid inhalation of vapors or spray mist.
  • Avoid contact with skin and eyes.
  • Keep away from sparks, hot surfaces, and open flames.
  • Follow all local and national health and safety regulations.

Always consult the Safety Data Sheet (SDS) before use.

Storage Recommendations 📦

Store HumiSeal® 1A27 LTX in tightly closed containers, away from excessive heat or cold. Recommended storage temperature is 0–35°C. Prior to use, allow the material to equilibrate for 24 hours at room temperature (18–32°C).


Compliance You Can Trust ✅

HumiSeal® 1A27 LTX meets stringent regulatory and performance standards for conformal coatings:

✔ GB30981-2020 compliant
✔ UL 94 V-0 flammability rated
✔ High dielectric strength and insulation resistance
✔ Designed for long-term electronic protection

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers