Hi-Flo Solder Bar Sn63Pb37

Harmonization Code : 3810.10.00 | Soldering, brazing or welding powders and pastes consisting of metal and other materials

Hi-Flo Solder Bar Sn63Pb37

Main features

  • Reduced Wave-Soldering Bridging and Icicling
  • Vaculoy Ultra-High-Purity Manufacturing
  • Conventional or Inert-Atmosphere Wave Soldering

Product Description

ALPHA® HiFlo Sn63Pb37 Wave Solder Bar is a high-fluidity tin-lead wave solder alloy manufactured using ultra-high-purity raw materials and Alpha's proprietary Vaculoy® process. The alloy is conditioned with viscosity- and dross-lowering treatments to minimize oxides, reduce dross generation, and deliver consistent soldering performance for conventional and inert-atmosphere wave soldering systems. It is engineered to improve solder joint quality while reducing bridging, icicling, skips, and solder pot maintenance.

Key Features

  • High-fluidity alloy that improves wetting while reducing bridging, icicling, and solder skips.
  • Ultra-high-purity composition produced using the Vaculoy® process to minimize oxides and dross formation.
  • Optimized for wave soldering in conventional and inert-atmosphere equipment, including densely populated PCB assemblies.

Applications / Suitable for

  • Wave soldering of through-hole assemblies
  • Wave soldering of mixed-technology PCB assemblies
  • Densely populated printed circuit boards
  • Fine-pitch electronic assemblies
  • Conventional and inert-atmosphere wave soldering systems
Product Family

HI-FLO Sn63Pb37 SOLDER BAR

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Method / Condition
Alloy Sn63/Pb37 — Nominal alloy composition
Tin (Sn) 62.5–63.5 wt% J-STD-006C / ISO 9453
Lead (Pb) Balance wt% J-STD-006C / ISO 9453
Recommended solder pot temperature 240–250 °C Wave soldering
Available forms 1 kg bars, 3.5 kg feeder bars, chunks — Published availability
Manufacturing process Vaculoy® high-purity process — Published product information