EPOXYLITE E6001 Hermetic Epoxy Impregnating Resin is a solvent-borne epoxy insulating varnish for dip-and-bake impregnation of motor windings used in hermetic compressors and refrigeration equipment. The clear amber liquid has 36 to 40% nonvolatile content, typical viscosity of 100 to 200 cP, and a flash point of 13 deg C. stated cure options include two hours at 77 deg C followed by six hours at 135 deg C, or 30 minutes at 177 deg C. The product supports winding impregnation where a low-viscosity epoxy varnish and controlled thermal cure are required.

Key features

  • Low-viscosity winding impregnation: Typical viscosity is 100 to 200 cP in the as-supplied clear amber liquid.
  • Controlled nonvolatile content: The varnish contains 36 to 40% nonvolatile material.
  • Heat-cure flexibility: Documented cure options include a staged 77/135 deg C cycle or 30 minutes at 177 deg C.

Applications

  • Motor-winding impregnation for hermetic compressors
  • Motor-winding impregnation for refrigeration units
  • Dip-and-bake insulating varnish applications

Technical Specifications

General Properties
Appearance Appearance
clear amber liquid
Physical Properties
Viscosity Viscosity
100-200 mPa.s
Thermal Properties
Flash Point Flash Point
13 °C
Electrical Properties
Dielectric Strength Dielectric Strength
157.48 kV/mm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied values for the solvent-borne epoxy insulating varnish.

Property Value Unit Method / condition
Appearance Clear amber liquid - As supplied
Nonvolatile content 36 to 40 % As supplied
Viscosity 100 to 200 cP As supplied
Weight per gallon 8.2 to 8.5 lb/gal As supplied
Flash point 13 deg C Equivalent to 55 deg F
Volatile organic content 5.2 lb/gal As supplied