EPOCAP 47577

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

EPOCAP 47577

Main features

  • UL 94 V-0 Classification
  • Non-Abrasive Filler for Automated Dispensing
  • 206-Minute Working Window

Product Description

EPOCAP® 47577/57577 (formerly EPOCAP® 17577) is a two-component, room temperature curing epoxy encapsulation system specifically designed for protecting submersible pump equipment. It features excellent cured properties and is formulated with non-abrasive inert fillers, making it well-suited for processing through automated dispensing equipment.

Key features

  • Flame retardant: Recognized to meet UL 94 V-0 flame retardancy standards at a thickness of 0.250".
  • Machine-friendly formulation: Contains non-abrasive inert fillers that minimize wear and facilitate ease of use in automated dispensing equipment.
  • Extended working time: Provides a long pot life with a gel time of 206 minutes for a 100-gram mass at 25°C, accommodating large or complex potting applications.

Applications / Suitable for

  • Encapsulation of submersible pump equipment.
  • General potting applications requiring UL 94 V-0 flame retardancy.
  • High-volume automated dispensing processes.
Product Family

EPOCAP 47577

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color Color
Black
Specific Gravity Specific Gravity
1.52 g/cm³
Physical Properties
Viscosity Viscosity
3,500 (Mixed) mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Pre-cure processing characteristics of mixed EPOCAP® 47577/57577.

Property Value Unit Method / condition
Appearance / Color (Mixed) Black - -
Mix Ratio (Weight) 100:13 - Part 47577 to Part 57577
Mix Ratio (Volume) 100:22 - Part 47577 to Part 57577
Viscosity (Mixed) 3,500 cps at 25°C
Specific Gravity (Mixed) 1.52 - at 25°C
Gel Time (100 gm mass) 206 minutes at 25°C
Gel Time (10 gm mass) 40 minutes at 60°C
Technical properties

After-processing / final-state properties

Typical cured mechanical, thermal, and electrical properties of EPOCAP® 47577/57577.

Property Value Unit Method / condition
Hardness 88 Shore D Tested at 25°C
Tensile Strength 6,150 psi Tested at 25°C
Compressive Strength 12,700 psi Tested at 25°C
Flexural Strength 10,700 psi Tested at 25°C
Linear Shrinkage 0.0011 in./in. Tested at 25°C
Heat Distortion Temperature 48 °C -
Recommended Service Temperature 105 °C -
UL Flame Retardancy Pass - UL 94 V-0 @ 0.250"
Dielectric Strength 378 volts/mil -