ENTHONE 77

Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other

ENTHONE 77

Main features

  • Ambient or Heat-Cure Choice
  • One-Hour Ink Pot Life
  • Heat-Enhanced Adhesion Development

Product Description

ENTHONE Catalyst 77 is an adhesion-promoting catalyst component for ENTHONE M-Series and 50-Series epoxy marking inks. It supports room-temperature or heat cure, with an average catalyzed-ink pot life of 1 hour after induction. At room temperature, the ink cures in 5 to 7 days; maximum adhesion is achieved with heat cure at 65.6 to 93.3 deg C. Catalyst 77 is used within matched ENTHONE ink systems for permanent markings on semiconductor components, printed circuit boards, connectors, dials, glass, metal, and thermosetting plastics.

Key features

  • Ambient or Heat Cure: Catalyst 77 supports room-temperature processing or controlled thermal cure.
  • One-Hour Pot Life: The catalyzed ink has an average 1-hour working pot life after induction.
  • Adhesion-Promoting Cure: Heat cure at 65.6 to 93.3 deg C develops maximum adhesion in the matched ink system.

Applications / Suitable for

  • ENTHONE M-Series epoxy marking inks
  • ENTHONE 50-Series epoxy marking inks
  • Permanent semiconductor and circuit-board marking systems

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical catalyst and catalyzed-ink processing data. Final properties belong to the selected ink, color, catalyst ratio, and cure schedule.

Property Value Unit Method / condition
Catalyst function Adhesion-promoting - For ENTHONE M-Series and 50-Series epoxy marking inks
Cure mode Room temperature or heat - Catalyst 77
Average pot life 1 hr Catalyzed ink; begins after induction period
Room-temperature cure 5 to 7 days Catalyzed ink system
Maximum-adhesion heat cure 65.6 to 93.3 deg C 150 to 200 deg F