ELANTAS TU-8040

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

ELANTAS TU-8040

Main features

  • 1:1 Controlled Mixing
  • 1,700 cP Mixed Viscosity
  • 700% Cured Elongation

Product Description

CONATHANE® TU-8040 Polyurethane Tooling Elastomer is an unfilled, two-component, room-temperature-curing, 100% solids polyurethane system for casting tough, highly extensible elastomeric parts. The light-yellow and light-amber components use a cartridge-friendly 1:1 mix ratio by weight and volume. The system is documented for detailed molds and sound-damping pads and has a typical initial mixed viscosity of 1,700 cP, 30-minute work life, and 60-minute gel time at 25°C. After cure, the material has Shore A 40 hardness, 700 psi tensile strength, and 700% elongation.

Key features

  • Cartridge-friendly 1:1 ratio: The two components mix 1:1 by weight and volume.
  • Low mixed viscosity: Typical initial mixed viscosity is 1,700 cP with a 30-minute work life.
  • Soft high-elongation elastomer: Typical cured properties include Shore A 40 hardness and 700% elongation.

Applications / Suitable for

  • Detailed mold casting
  • Sound-damping pads
  • Tough flexible polyurethane castings

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or processing-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Part A viscosity 3,000 cP At 25°C
Part B viscosity 300 cP At 25°C
Part A specific gravity 1.07 N/A At 25°C
Part B specific gravity 1.07 N/A At 25°C
Mix ratio 1:1 ratio By weight and volume
Initial mixed viscosity 1,700 cP At 25°C
Work life 30 min At 25°C
Gel time 60 min At 25°C
Technical properties

After-processing / final-state properties

Typical cured or final-state values under the stated system and test conditions. These values are not sales specifications.

Property Value Unit Method / condition
Hardness 40 Shore A ASTM D2240
Tensile strength 700 psi ASTM D412
Ultimate elongation 700 % ASTM D412
Graves tear strength 90 pli ASTM D412
Bashore rebound 59 % ASTM D2632

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers