ELANTAS TU-79MF

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

ELANTAS TU-79MF

Main features

  • Abrasion-Resistant Polyurethane Tooling Elastomer
  • 4,000 cP Mixed Viscosity
  • 1,800 psi Cured Tensile Strength

Product Description

CONATHANE® TU-79MF Polyurethane Tooling Elastomer is an unfilled, two-component, room-temperature-curing, 100% solids polyurethane system for casting and potting abrasion-resistant elastomeric parts. The clear light-amber system is documented for metal-polishing and finishing linings, industrial wheels, metal-forming pads, flexible molds, washers, gaskets, bushings, and vibration, shock, or sound-damping pads. It uses a 100:45 mix ratio by weight or volume and has a typical initial mixed viscosity of 4,000 cP with a 25 to 35-minute work life. Typical cured properties include Shore A 78 hardness and 750% elongation.

Key features

  • Abrasion-resistant tooling elastomer: The system is documented for linings, wheels, molds, gaskets, and damping pads.
  • Controlled casting process: Typical mixed viscosity is 4,000 cP with a 25 to 35-minute work life.
  • Highly extensible cured material: Typical cured elongation is 750% with Shore A 78 hardness.

Applications / Suitable for

  • Metal-polishing and finishing linings
  • Industrial wheels, forming pads, and flexible molds
  • Washers, gaskets, bushings, and damping pads

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or processing-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Part A viscosity 5,000 cP At 25°C
Part B viscosity 1,500 cP At 25°C
Part A specific gravity 1.07 N/A At 25°C
Part B specific gravity 1.08 N/A At 25°C
Mix ratio 100:45 parts by weight Part A : Part B
Initial mixed viscosity 4,000 cP At 25°C
Work life 25 to 35 min At 25°C
Cure options 7 days at 25°C; 1 h at 25°C plus 16 h at 80°C N/A Documented schedules
Technical properties

After-processing / final-state properties

Typical cured or final-state values under the stated system and test conditions. These values are not sales specifications.

Property Value Unit Method / condition
Hardness 78 Shore A ASTM D2240
Tensile strength 1,800 psi ASTM D412
Ultimate elongation 750 % ASTM D412
Graves tear strength 325 pli ASTM D412
Linear shrinkage <0.5 % Cured at 25°C
Compression set 28 % ASTM D395 Method B