ELANTAS K-22

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

ELANTAS K-22

Main features

  • Metal, Rubber, and Wood Bonding
  • 20-Minute Working Window
  • 2,500 psi Shear Strength

Product Description

EASYPOXY® K-22 Epoxy Adhesive is a black, two-component, 100% solids epoxy adhesive and repair compound for metal, wood, rubber, and many plastic substrates. The paste system cures at room temperature or with low heat and is supplied for general-purpose bonding, repair, and sealing. Published portfolio data identify a 100:45 mix ratio by weight, approximately 20-minute pot life, and typical shear strength of 2,500 psi. The cured epoxy is electrically insulating and is intended for assemblies where the bonded materials may have different coefficients of thermal expansion.

Key features

  • General-purpose epoxy adhesive: The two-part paste bonds metal, wood, rubber, and many plastics.
  • Room-temperature or low-heat cure: The 100% solids system supports flexible cure planning.
  • Published 2,500 psi shear strength: Portfolio data identify a 100:45 mix ratio and approximately 20-minute pot life.

Applications / Suitable for

  • Metal bonding and repair
  • Wood and rubber bonding
  • Bonding many plastic substrates
Product Family

ELANTAS K-22

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or processing-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Product form Two-component epoxy paste N/A As supplied
Color Black N/A As supplied
Solids content 100 % System description
Mix ratio 100:45 parts by weight Resin : hardener
Pot life 20 min Published portfolio value
Cure method Room temperature or low heat N/A Documented