ELANTAS EN-2553

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

ELANTAS EN-2553

Main features

  • Filled Flame-Retardant Polyurethane Potting System for Components
  • 4,500 cP Mixed Viscosity
  • UL 94 V-0 Classification

Product Description

CONATHANE® EN-2553 Polyurethane Encapsulant is a two-component, filled, flame-retardant polyurethane potting system for electronic components, modules, circuit boards, assemblies, and related devices. The brown Part A and black or blue Part B are mixed at 17:100 by weight to produce a typical initial viscosity of 4,500 cP and a 55-minute work life at 25°C. The system is documented for low-stress cure and thermal-shock resistance, with cure options of seven days at 25°C or 16 hours at 80°C. Typical cured properties include Shore A 95 hardness, 60% elongation, and UL 94 V-0 at 3 mm.

Key features

  • Filled flame-retardant polyurethane: The cured material is documented as UL 94 V-0 at 3 mm.
  • 55-minute work life: Typical initial mixed viscosity is 4,500 cP at 25°C.
  • Low-stress protection: The system is documented for sensitive components and thermal-shock resistance.

Applications / Suitable for

  • Electronic components and modules
  • Circuit boards and assemblies
  • Low-stress encapsulation of sensitive devices

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or processing-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Part A viscosity 300 cP At 25°C
Part B viscosity 8,500 cP At 25°C
Part A specific gravity 1.24 N/A At 25°C
Part B specific gravity 1.49 N/A At 25°C
Mix ratio 17:100 parts by weight Part A : Part B
Initial mixed viscosity 4,500 cP At 25°C
Work life 55 min At 25°C
Cure options 7 days at 25°C; 16 h at 80°C N/A Documented schedules
Technical properties

After-processing / final-state properties

Typical cured or final-state values under the stated system and test conditions. These values are not sales specifications.

Property Value Unit Method / condition
Hardness 95 Shore A ASTM D2240
Tensile strength 1,050 psi ASTM D412
Ultimate elongation 60 % ASTM D412
Tear strength 140 pli ASTM D624
Dielectric strength 560 V/mil ASTM D149
Volume resistivity 3.1 × 10¹⁴ ohm·cm ASTM D257 at 25°C
Flammability classification V-0 UL 94 At 3.0 mm