ELANTAS CE-1171

Harmonization Code : 3404.90.00.00 | Artificial waxes and prepared waxes : Other

ELANTAS CE-1171

Main features

  • Transparent Conformal Coating
  • 20-Minute Tack-Free Time
  • 900 cP Application Viscosity

Product Description

CONAP® CE-1171 Acrylic Conformal Coating is a transparent, solvent-based, single-component acrylic conformal coating for electrical insulation and moisture protection of printed circuitry and electronic components. The amber coating may be sprayed, dipped, or brushed and includes a tracer dye for ultraviolet inspection. It is documented for flexibility, reparability, hydrolytic stability, and adhesion to phenolic and epoxy-glass laminates in adverse environments. Typical as-supplied properties include 900 cP viscosity, 30% solids, 0.98 specific gravity, and a 20-minute tack-free time, with full cure in 24 hours at 25°C.

Key features

  • Single-component acrylic coating: The transparent solvent-based coating supports spray, dip, and brush application.
  • Fast handling: Typical tack-free time is 20 minutes with full cure in 24 hours at 25°C.
  • UV inspection tracer: The coating includes a tracer dye for inspection under ultraviolet light.

Applications / Suitable for

  • Printed circuit-board protection
  • Thin-film coating of electronic components
  • Phenolic and epoxy-glass laminate assemblies

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or processing-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Product form Single-component acrylic coating N/A As supplied
Color Amber, slight haze N/A As supplied
Viscosity 900 cP At 25°C
Specific gravity 0.98 N/A At 25°C
Solids content 30 % 135°C for 45 min
Flash point 18 °C ASTM D93
Tack-free time 20 min Typical
Full cure 24 h At 25°C