ELANTAS AD-1147

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

ELANTAS AD-1147

Main features

  • Heat-Activated Surface Preparation Cure
  • Metals, Glass, Glass-Fiber Laminates, Wood, and Leather
  • 2,000 cP Application Viscosity

Product Description

CONAP® AD-1147 Adhesive Primer is a high-strength, solvent-borne adhesive primer for bonding liquid polyurethane compounds to inorganic and organic substrates during cure. The amber polymer solution is documented for aluminum alloys, magnesium, iron, steel, glass, glass-fiber laminates, wood, and leather. It may be applied by brush, spray, roller coating, or doctor blade and requires heat activation before the liquid urethane is introduced. Typical as-supplied properties include 2,000 cP viscosity, 24% solids content, and 0.90 specific gravity at 25°C.

Key features

  • Liquid-urethane bonding primer: The primer is formulated to bond polyurethane compounds to prepared substrates during cure.
  • Broad substrate coverage: Documented substrates include metals, glass, glass-fiber laminates, wood, and leather.
  • Heat-activated film: The applied primer is activated by baking for one to two hours at 82°C to 93°C.

Applications / Suitable for

  • Priming metals for liquid polyurethane bonding
  • Priming glass and glass-fiber laminates
  • Priming wood and leather for polyurethane overmolding

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or processing-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Product form Solvent-borne adhesive primer N/A As supplied
Color Amber N/A As supplied
Viscosity 2,000 cP At 25°C
Solids content 24 % Typical
Specific gravity 0.90 N/A At 25°C
Shelf stability 15 months Original unopened container
Air-dry time ≥1 h After final coat
Activation bake 1 to 2 h At 82°C to 93°C