LOCTITE ECCOBOND UV9060F

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

LOCTITE ECCOBOND UV9060F

Main features

  • UV & Moisture Cure
  • Cures in shadowed areas
  • Translucent light blue

Product Description

LOCTITE ECCOBOND UV 9060F no flow encapsulant is designed for local circuit board protection as a UV curing coating/encapsulant with secondary moisture cure in shadow areas. This product is fluorescent when viewed with ultraviolet (black) light.

LOCTITE ECCOBOND UV 9060F is a one component, fast curable translucent material that is easily dispensed without stringing. It is fluorescent under UV light and it typically used for assembly applications and the local protection of WLCSP and BGA on circuit boards.

Technical Specifications

Thermal Properties
Glass Transition Temperature (Tg) Glass Transition Temperature (Tg)
75 °C
Physical Properties
Viscosity Viscosity
11,000 mPa.s

Additional Information

UV Cure

Light Source and Condition:

Metal halide doped spectrum UV lamp

  • Lamp Power, W/in 300
  • Distance between lamp to substrate, inches 4
  • Irradiance UVA, EIT puck radiometer, mW/cmÇ 566
  • Recommended Dose, seconds 5 to 25

Moisture cure occurs at ambient temperature and humidity.

*Cures at least 0.25 inch under optimum conditions.