LOCTITE ECCOBOND ME995-1-4

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE ECCOBOND ME995-1-4

Main features

  • One component
  • Thermally conductive
  • High viscosity

Product Description

LOCTITE ABLESTIK ME 995-1-4 is a thermally conductive, glob top epoxy for microelectronics applications. It offers high viscosity and medium thixotropy and is typically used as a non conductive adhesive.

 

Cure Schedule

  • 60 minutes @ 150°C or
    40 minutes @ 170°C or
    20 minutes @ 190°C

 

Technical Specifications

General Properties
Density (g) Density (g)
1.5 g/cm3
Pot Life Pot Life
72 hours
Physical Properties
Viscosity Viscosity
335,000 mPa.s
Thermal Properties
Glass Transition Temperature (Tg) Glass Transition Temperature (Tg)
110 °C
Thermal Conductivity Thermal Conductivity
0.5 W/m.K