ECCOBOND LUX OGR146TUV

Harmonization Code : 38159000 | Unspecified reaction initiators, accelerators, and catalytic preparations

ECCOBOND LUX OGR146TUV

Main features

  • UV and Shadow-Area Thermal Cure
  • Low-Refractive-Index Optical Bonding
  • Extended 91-Day Working Window

Product Description

LOCTITE ECCOBOND LUX OGR146TUV is a one-part photocurable acrylate adhesive for optical devices, fiber-optic assemblies, and optoelectronic components. UV exposure provides the primary cure, and secondary thermal schedules of 1 hour at 100 deg C or 2 hours at 85 deg C address material in shadowed areas after light curing. The cured adhesive has a low refractive index across multiple optical wavelengths, including 1.464 at 589 nm and 1.454 at 1550 nm. A 91-day work life at 25 deg C supports extended process availability for controlled, high-throughput assembly.

Key features

  • UV and Thermal Dual Cure: UV cure is supplemented by defined thermal schedules for adhesive in shadowed areas.
  • Low Refractive Index: Cured refractive index ranges from 1.464 at 589 nm to 1.454 at 1550 nm.
  • Extended Work Life: A 91-day work life at 25 deg C supports long process availability before cure.

Applications / Suitable for

  • Optical devices
  • Fiber-optic assembly
  • Optoelectronic assembly
  • High-throughput optical assembly

Technical Specifications

General Properties
Color Color
Colorless
Physical Properties
Viscosity Viscosity
1,250 mPa.s
Other Properties
Storage Temperature Storage Temperature
-5 to +5 °C
Thermal Properties
Glass Transition Temperature (Tg) Glass Transition Temperature (Tg)
77 °C

Additional Information

Technical properties

As-supplied / before-processing properties

As-supplied and processing characteristics used for material and process evaluation. Numerical values are typical unless otherwise identified.

Property Value Unit Method / condition
Chemical class Acrylate - As supplied
Component count One-part - As supplied
Work life 91 days At 25 deg C
Primary cure wavelength 365 nm UV light
Secondary thermal cure 1 hour at 100 deg C or 2 hours at 85 deg C - After light cure for shadowed areas
Technical properties

After-processing / final-state properties

Final-state characteristics after the stated cure or processing condition. Numerical values are typical unless otherwise identified.

Property Value Unit Method / condition
Refractive index 1.464 - At 589 nm
Refractive index 1.458 - At 830 nm
Refractive index 1.454 - At 1550 nm
Tensile modulus 635 N/mm^2 DMTA at 25 deg C
Moisture absorption at saturation 1.7 wt.% 85 deg C and 85% RH