LOCTITE ECCOBOND FP4527

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

LOCTITE ECCOBOND FP4527

Main features

  • Low viscosity
  • High flow
  • Excellent wettability

Product Description

LOCTITE® ECCOBOND FP4527 epoxy underfill has excellent wettability and is typically used on a semiconductor level as a capillary underfill.

LOCTITE® ECCOBOND FP4527 is a low viscosity, high flow, epoxy based material designed for capillary underfill on flip chip applications.

Cure Schedule

  • 15 minutes @ 165°C (hot plate) 
  • 30 minutes @ 165°C (convection)
  • 1hour @110°C + 30 minutes @150°C (convection) 
Product Family

ECCOBOND FP4527

1. Select Package Type

Loading pricing…

Product availability
US Shipping in 94 days
CA Shipping in 12 weeks
EU Shipping in 95 days
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Filler Content Filler Content
68 %
Pot Life Pot Life
48 hours
Thermal Properties
Glass Transition Temperature (Tg) Glass Transition Temperature (Tg)
158 °C
Chemical Properties
Moisture absorption Moisture absorption
1.5 %
Physical Properties
Viscosity Viscosity
12,000 mPa.s