LOCTITE ECCOBOND FP4451

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

LOCTITE ECCOBOND FP4451

Main features

  • Encapsulant - DAM
  • High purity
  • Minimal slumping

Product Description

LOCTITE ECCOBOND FP4451 is the industry standard damming material, designed as a flow control barrier around areas of bare chip encapsulation.

LOCTITE ECCOBOND FP4451 is designed to be used in combination with FP4450 fill encapsulant. It passes pressure pot performance on live devices up to 500 hours with no failures depending on device and package type.

Recommended Cure Schedule
  • 30 minutes @ 125°C plus
  • 90 minutes @ 165°C

Technical Specifications

General Properties
Pot Life Pot Life
48 hours
Specific Gravity Specific Gravity
1.76
Thermal Properties
Glass Transition Temperature (Tg) Glass Transition Temperature (Tg)
155 °C
Other Properties
MSL Level MSL Level
MSL 2
Physical Properties
Viscosity Viscosity
1,300,000 mPa.s