LOCTITE ECCOBOND D125 F DR

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

LOCTITE ECCOBOND D125 F DR

Main features

  • Low water absorption
  • Low exotherm
  • Non-sag

Product Description

LOCTITE D 125 F DR is a epoxy surface-mount adhesive designed for high-speed dispensing.

LOCTITE D 125 F DR is used in a wide array of applications, including chip capacitors, chip resistors, SOTs, SOICs, and PLCCs. 

 

Product Family

ECCOBOND D125

Loading pricing…

Technical Specifications

General Properties
Specific Gravity Specific Gravity
1.275
Thermal Properties
Glass Transition Temperature (Tg) Glass Transition Temperature (Tg)
85 °C
Thermal Conductivity Thermal Conductivity
0.3 W/m.K
Electrical Properties
Volume Resistivity Volume Resistivity
1000000000000000 Ohms⋅cm

Additional Information

TYPICAL CURING PERFORMANCE 

IR or Convection Conveyor Oven
20 minutes @ 100°C
7 minutes @ 110°C
2.5 minutes @ 120°C
1.5 minutes @ 150°C

Convection Box Oven

30 minutes @ 100°C
20 minutes @ 110°C
10 minutes @ 120°C 
5 minutes @ 150°C

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers