LOCTITE ECCOBOND 50300-1

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

LOCTITE ECCOBOND 50300-1

Main features

  • One component
  • Low CTE
  • Low viscosity

Product Description

LOCTITE ECCOBOND 50300-1 glob top is designed for encapsulating wire bonded bare die on epoxy laminate and similar substates. The formulation of this single component material ensures a long pot and a very stable viscosity during use.

LOCTITE ECCOBOND 50300-1 is recommended for use on ICs with high wire profiles and in applications where the spreading of the glob top during cure must be controlled. It is a 70% filled product with 100% solids by weight.

Cure Schedule

  • 2 hours @ 150°C

Low Stress Cure Schedule

  • 1 hour @ 120°C + 1 hour @ 150°C

For best results, substrate should be preheated (up to a maximum of 70ºC) to obtain the optimum flow under and around the wires.

Technical Specifications

General Properties
Pot Life Pot Life
168 hours
Thermal Properties
Glass Transition Temperature (Tg) Glass Transition Temperature (Tg)
140 °C
Thermal Conductivity Thermal Conductivity
0.63 W/m.K
Electrical Properties
Volume Resistivity Volume Resistivity
330000000000000 Ohms⋅cm
Chemical Properties
Water Absorption Water Absorption
0.4 %
Physical Properties
Viscosity Viscosity
100 mPa.s