Main features

  • Flexible Low-Modulus Protection
  • Light and Shadow-Area Cure
  • Fluorescent Conformal-Coverage Inspection

Product Description

Dymax Multi-Cure 9-20557 Flexible Light-Cure Conformal Coating is a single-component, medium-viscosity conformal coating for printed circuit boards and electronic assemblies. UV or visible light cures exposed areas, while secondary heat cure develops coating in shadowed regions. The flexible, low-modulus cured film provides protective coverage without the rigidity of a bulk encapsulant. Blue fluorescence supports inspection, and the coating can be applied across metal, ceramic, PCB, flex, and silicon surfaces. Its solvent-free acrylated urethane form avoids component mixing and supports controlled dispensing.

Key features

  • Flexible Low-Modulus Protection: The cured film combines conformal coverage with a flexible mechanical profile.
  • Light Plus Shadow-Area Cure: UV or visible light cure is complemented by secondary heat cure in shaded regions.
  • Blue-Fluorescent Inspection: Fluorescence under black light supports coating coverage checks.

Applications / Suitable for

  • Conformal coating of printed circuit boards
  • Conformal coating of electronic assemblies
Product Family

DYMAX 9-20557

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance Appearance
Clear to Light Yellow
Chemistry Type Chemistry Type
Acrylated Urethane
Refractive index Refractive index
1.51
Physical Properties
Viscosity Viscosity
2,300 mPa.s
Mechanical Properties
Elongation Elongation
110 %
Chemical Properties
Water Absorption Water Absorption
1.0 %
Other Properties
Storage Temperature Storage Temperature
10 - 32 °C

Additional Information

Technical properties

As-supplied / before-processing properties

As-supplied characteristics used for material and process evaluation. Numerical values are typical unless otherwise identified.

Property Value Unit Method / condition
Solvent content No nonreactive solvents - As supplied
Chemical class Acrylated urethane - As supplied
Appearance Clear to light yellow - As supplied
Density 1.05 g/ml ASTM D1875
Viscosity 2,300 nominal cP ASTM D1084; 20 rpm
Shelf life 12 months Original unopened container; store at 10 to 32 deg C
Technical properties

After-processing / final-state properties

Final-state characteristics after the stated cure or processing condition. Numerical values are typical unless otherwise identified.

Property Value Unit Method / condition
Durometer hardness D60 - ASTM D2240
Tensile strength at break 10 (1,500) MPa (psi) ASTM D638
Elongation at break 110 % ASTM D638
Modulus of elasticity 89 (13,000) MPa (psi) ASTM D638
Boiling water absorption 2.7 % ASTM D570; 2 hr
Water absorption 1.0 % ASTM D570; 25 deg C for 24 hr
Dielectric withstand voltage >1,500 V MIL-I-46058C
Volume resistivity 1.48 x 10^15 ohm cm ASTM D257