DYMAX 3019

Harmonization Code : 3824.99.92.97 | Prepared binders for foundry molds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included: other : other : other

DYMAX 3019

Main features

  • Fast UV/Visible-Light Plastic Bonding
  • Moisture-Resistant Clear Bond Lines
  • Fluorescent In-Line Inspection

Product Description

Dymax Ultra Light-Weld 3019 Series Moisture-Resistant Adhesives are UV- and visible-light-curable adhesives for fast bonding of flexible and rigid plastic substrates. The 100% reactive-solids, solvent-free formulations form clear bond lines on materials including polycarbonate, PVC, polyurethane, PET, PETG, polystyrene, and nylon. The series includes a nominal 450 mPa s 3019 liquid and a 25,000 mPa s 3019-GEL grade for different dispensing requirements. After cure, typical series properties include Shore D55 hardness, 1,700 psi tensile strength, and 170% elongation at break. The adhesives also fluoresce under low-intensity 365 nm black light, supporting in-line inspection of dispensed and bonded areas.

Key features

  • Fast light-activated bonding: UV or visible light develops bonds in seconds under validated exposure conditions.
  • Liquid and gel viscosities: The series includes nominal 450 mPa s and 25,000 mPa s grades for different dispensing needs.
  • Fluorescent inspection: The adhesive fluoresces under low-intensity 365 nm black light.

Applications / Suitable for

  • Polycarbonate and PVC bonding
  • Polyurethane, PET, and PETG bonding
  • Polystyrene and nylon bonding
Product Family

DYMAX 3019

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance Appearance
Clear/Light Amber Liquid
Refractive index Refractive index
1.48
Thermal Properties
Flash Point Flash Point
>93 °C
Chemical Properties
Water Absorption Water Absorption
2.1 %

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied properties for the 3019 Series; viscosity depends on grade.

Property Value Unit Method / condition
Solvent content None 100% reactive solids
Appearance Clear to light amber As supplied
Refractive index 1.48 At 20 deg C
Density 1.05 g/mL Typical
3019 viscosity 450 mPa s Nominal; ASTM D1084
3019-GEL viscosity 25,000 mPa s Nominal; ASTM D2556
Shelf life 12 months Unopened container
Storage temperature 10 to 32 deg C Unopened container
Technical properties

After-processing / final-state properties

Typical cured properties for the 3019 Series.

Property Value Unit Method / condition
Durometer hardness 55 Shore D Cured material
Tensile strength 1,700 psi Cured material
Elongation at break 170 % Cured material
Modulus of elasticity 30,000 psi Cured material
Water absorption 2.1 % 24 hours
Boiling-water absorption 1.3 % 2 hours
Linear shrinkage 3.0 % After cure

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers