DOWSIL X3-1598

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

DOWSIL X3-1598

Main features

  • UV-Indicator Flowable Silicone Adhesive
  • 60-Minute 125 deg C Cure
  • Primerless Aluminum Bonding

Product Description

DOWSIL™ X3-1598 Adhesive is a one-part, black, flowable heat-cure silicone adhesive with high tensile strength and a UV indicator for automated inspection. The ready-to-use material contains no added solvents and may be applied by manual or automated needle dispensing. Documented applications include sealing lids and housings, attaching baseplates, gasketing, connector sealing, engine and transmission controllers, ABS assemblies, and lighting. Typical viscosity is 86,550 cP, with cure schedules of 60 minutes at 125°C or 30 minutes at 150°C. Typical lap shear adhesion to unprimed aluminum is 5.8 MPa.

Key features

  • UV inspection indicator: The black adhesive includes an indicator for automated inspection.
  • One-part heat cure: Documented cure schedules are 60 minutes at 125°C or 30 minutes at 150°C.
  • Strong aluminum adhesion: Typical unprimed lap shear adhesion to aluminum is 5.8 MPa.

Applications / Suitable for

  • Sealing lids, housings, and connectors
  • Attaching baseplates and gasketing
  • Engine, transmission, ABS, and lighting assemblies

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or processing-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Product form One-part flowable adhesive N/A As supplied
Color Black N/A As supplied
Viscosity 86,550 cP Typical
Heat-cure option 60 min At 125°C
Heat-cure option 30 min At 150°C
Shelf life 12 months At 5°C
Technical properties

After-processing / final-state properties

Typical cured, installed, or in-use values under the stated conditions. These values are not sales specifications.

Property Value Unit Method / condition
Cured specific gravity 1.32 N/A Typical cured value
Lap shear adhesion 5.8 MPa Unprimed aluminum
Dielectric strength 22 kV/mm Typical cured value

Leading Brands Trust in Our Products and Services