Main features

  • One-Part No-Mix Bonding
  • 30-Minute 150 deg C Cure
  • 1,030 psi Cured Tensile Strength

Product Description

DOWSIL™ SE 1714 Adhesive is a one-part, black or beige, flowable addition-cure silicone adhesive and sealant for electronics and automotive assemblies. The ready-to-use material requires no mixing and is heat cured above 100°C, with a typical cure condition of 30 minutes at 150°C. Documented applications include sealing lids and housings for electronic control units and power modules, fixing printed circuit-board and system assemblies, and reinforcing connector components. Typical cured properties include Shore A 65 hardness, 1,030 psi tensile strength, 250% elongation, and a specific gravity of 1.3 at 25°C.

Key features

  • One-part flowable adhesive: The ready-to-use material can flow, fill, or self-level after dispensing.
  • Heat-cure processing: A typical cure condition is 30 minutes at 150°C.
  • Strong cured elastomer: Typical data include 1,030 psi tensile strength and 250% elongation.

Applications / Suitable for

  • Sealing lids and housings for ECUs and power modules
  • Fixing PCB and system assemblies
  • Reinforcing or fixing connector components
Product Family

DOWSIL SE1714

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or processing-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Product form One-part flowable adhesive / sealant N/A As supplied
Color Black or beige N/A As supplied
Cure type Addition cure N/A Heat cure above 100°C
Typical cure 30 min At 150°C
Technical properties

After-processing / final-state properties

Typical cured, installed, or in-use values under the stated conditions. These values are not sales specifications.

Property Value Unit Method / condition
Specific gravity 1.3 N/A At 25°C
Hardness 65 Shore A Typical cured value
Tensile strength 1,030 psi Typical cured value
Elongation 250 % Typical cured value