Main features

  • 10-Minute Tack-Free Time
  • 2.9 MPa Cured Tensile Strength
  • UL 94 V-0 Classification

Product Description

DOWSIL™ SE 9188 RTV Adhesive is a one-part, gray, non-flowing polydimethylsiloxane adhesive for room-temperature bonding, fixing, vibration dampening, and sealing in electronics assemblies. The material requires no mixing and has a typical tack-free time of 10 minutes at 25°C, with optional mild heat acceleration. It is documented with controlled silicone volatility and a UL 94 V-0 flammability classification. Typical cured properties include Shore A 34 hardness, 2.9 MPa tensile strength, 400% elongation, 30 kV/mm dielectric strength, and 1.0 × 10¹⁵ ohm·cm volume resistivity.

Key features

  • Non-flowing one-part RTV: The gray adhesive remains in place and requires no component mixing.
  • Fast tack-free cure: Typical tack-free time is 10 minutes at 25°C.
  • Documented flame classification: The product is listed with UL 94 V-0 flammability classification.

Applications / Suitable for

  • Part fixing on circuit boards
  • Vibration dampening
  • Electronic sealing applications

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or processing-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Product form One-part non-flowing RTV adhesive N/A As supplied
Color Gray N/A As supplied
Tack-free time 10 min At 25°C
Low-molecular siloxane content 30 ppm D4-D10
Low-molecular siloxane content 220 ppm D4-D20
Technical properties

After-processing / final-state properties

Typical cured, installed, or in-use values under the stated conditions. These values are not sales specifications.

Property Value Unit Method / condition
Cured specific gravity 1.29 N/A Typical cured value
Hardness 34 Shore A Typical cured value
Tensile strength 2.9 MPa Typical cured value
Elongation 400 % Typical cured value
Dielectric strength 30 kV/mm Typical cured value
Volume resistivity 1.0 × 10¹⁵ ohm·cm Typical cured value
Dielectric constant 3.4 N/A At 1 MHz
Flammability classification V-0 UL 94 Documented classification