DOWSIL SE1720

Main features

  • 1:1 Controlled Mixing
  • 89,700 cP Mixed Viscosity
  • 50-Minute 70 deg C Cure

Product Description

DOWSIL™ SE 1720 CV Adhesive Kit is a two-part, white, flowable silicone adhesive with a 1:1 mix ratio and controlled volatility for electronic assembly processes. The solvent-free material may be dispensed manually or automatically and has a typical mixed viscosity of 89,700 cP with a six-hour working time at 25°C. Documented cure schedules range from 50 minutes at 70°C to 10 minutes at 100°C. Applications include sealing ceramic condensers and printed circuit-board module components and bonding computer keypad assemblies. Typical cured properties include 3.3 MPa tensile strength, 375% elongation, and Shore A 33 hardness.

Key features

  • Flowable 1:1 system: The two-part adhesive supports manual or automated needle dispensing.
  • Moderate-temperature cure: Documented cure schedules range from 50 minutes at 70°C to 10 minutes at 100°C.
  • Controlled-volatility elastomer: Typical cured data include 3.3 MPa tensile strength and 375% elongation.

Applications / Suitable for

  • Sealing ceramic condensers
  • Sealing printed circuit-board module components
  • Bonding computer keypad assemblies
Product Family

DOWSIL SE 1720

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or processing-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Color White N/A As supplied
Mix ratio 1:1 ratio Part A : Part B
Viscosity, Part A 37,700 cP Typical
Viscosity, Part B 41,900 cP Typical
Mixed viscosity 89,700 cP Typical
Working time 6 h At 25°C
Heat cure 50 min at 70°C; 30 min at 80°C; 10 min at 100°C N/A Documented schedules
Technical properties

After-processing / final-state properties

Typical cured, installed, or in-use values under the stated conditions. These values are not sales specifications.

Property Value Unit Method / condition
Cured specific gravity 1.06 N/A Typical cured value
Tensile strength 3.3 MPa Typical cured value
Elongation 375 % Typical cured value
Tensile modulus 0.9 MPa Typical cured value
Hardness 33 Shore A JIS
Lap shear adhesion 1.6 MPa Unprimed aluminum