DOWSIL RSN-0996

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

DOWSIL RSN-0996

Main features

  • Motor/Coil/Transformer Impregnating Varnish
  • 150 deg C Minimum Cure Temperature
  • 1,626 V/mil Dielectric Strength

Product Description

DOWSIL™ RSN-0996 Resin is a clear-blue silicone resin in xylene used as a general-purpose impregnating varnish for motors, coils, and transformers. The varnish is documented for cure temperatures as low as 150°C and for long service at a 220°C hottest-spot temperature. It combines electrical properties, bond strength, moisture resistance, and a drainage profile intended to limit runoff during cure. Typical published data identify a relative density of 1.00 to 1.02 and dielectric strength of 1,626 V/mil, while the exact current technical data sheet should be confirmed before publication.

Key features

  • General-purpose impregnating varnish: The silicone resin is documented for motors, coils, and transformers.
  • Elevated-temperature service: The varnish may cure from 150°C and is documented for long service at a 220°C hottest-spot temperature.
  • Electrical insulation: Published typical data identify dielectric strength of 1,626 V/mil.

Applications / Suitable for

  • Motor winding impregnation
  • Coil impregnation
  • Transformer varnishing
Product Family

DOWSIL RSN-0996

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or processing-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Product form Silicone resin varnish N/A As supplied
Color Clear blue N/A As supplied
Solvent Xylene N/A As supplied
Relative density 1.00 to 1.02 N/A Published typical range
Technical properties

After-processing / final-state properties

Typical cured, installed, or in-use values under the stated conditions. These values are not sales specifications.

Property Value Unit Method / condition
Dielectric strength 1,626 V/mil Published typical value
Minimum documented cure temperature 150 °C Product overview
Hottest-spot service temperature 220 °C Documented long-service reference