DOWSIL RSN-0994

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

DOWSIL RSN-0994

Main features

  • Heat-Resistant Electrical Varnish
  • At Least 49% Solids
  • AIEE Class 220 deg C Insulation

Product Description

DOWSIL™ RSN-0994 Resin is a light-straw silicone electrical varnish in xylene for coating glass cloth and sleeving and for bonding mica-glass combinations. The material is documented as heat resistant, water repellent, and suitable as an AIEE Class 220°C insulating material. Glass cloth coated with the varnish retains flexibility and electric strength during extended high-temperature exposure under the stated test conditions. Typical as-supplied properties include at least 49% solids content, 80 to 150 mm²/s viscosity at 25°C, and 1.00 to 1.02 relative density.

Key features

  • Electrical insulating varnish: The silicone resin is documented for glass cloth, sleeving, and mica-glass bonding.
  • Heat and water resistance: The material is identified as an AIEE Class 220°C insulating material.
  • Controlled solvent-borne properties: Typical data include at least 49% solids and 80 to 150 mm²/s viscosity at 25°C.

Applications / Suitable for

  • Coating glass cloth
  • Coating electrical sleeving
  • Bonding mica-glass combinations
Product Family

DOWSIL RSN-0994

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or processing-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Physical nature Liquid N/A As supplied
Color Light straw N/A As supplied
Solids content ≥49 % Typical minimum
Viscosity 80 to 150 mm²/s At 25°C
Relative density 1.00 to 1.02 N/A At 25°C
Solvent Xylene N/A As supplied
Flash point 27 °C Closed cup
Technical properties

After-processing / final-state properties

Typical cured, installed, or in-use values under the stated conditions. These values are not sales specifications.

Property Value Unit Method / condition
Heat endurance, flex life 1,000 h At 250°C
Heat endurance, craze life 10,000 h At 250°C
Heat endurance, flex life 400 h At 300°C
Heat endurance, craze life 750 h At 300°C
Thermal life 9,000 h At 250°C
Thermal life 3,000 h At 275°C
Thermal life 800 h At 300°C