DOWSIL Q2-3067

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

DOWSIL Q2-3067

Main features

  • One-Part Grease-Like Optical Couplant
  • Fiber-Optic Assembly Applications
  • Above 101.1 deg C Flash Point

Product Description

DOWSIL™ Q2-3067 Optical Couplant is a one-part, amber, grease-like silicone optical couplant used to improve light transmission between optical interfaces. The non-curing material is documented for reducing reflection and intensity loss while improving sensitivity in fiber-optic, electro-optic, lens, and light-sensing assemblies. It combines high clarity with shear stability and remains usable for low-temperature coupling applications. Typical product data include a specific gravity of 0.976 at 25°C and a flash point above 101.1°C, and the material may be applied by blade, syringe, or compatible dispensing equipment.

Key features

  • Optical interface coupling: The grease-like silicone reduces reflection and intensity loss between optical components.
  • High clarity and shear stability: The material is documented for light-transmission and device-sensitivity applications.
  • Non-curing one-part format: The couplant is supplied ready to apply without mixing or cure processing.

Applications / Suitable for

  • Fiber-optic assemblies
  • Electro-optic systems and lens assemblies
  • Light-sensing instruments

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or processing-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Product form Grease-like optical couplant N/A As supplied
Components One-part N/A As supplied
Color Amber N/A As supplied
Specific gravity 0.976 N/A At 25°C
Flash point >101.1 °C Product listing
Application methods Blade, syringe, or dispensing equipment N/A Documented processing methods