DOWSIL PR1204

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

DOWSIL PR1204

Main features

  • Adhesion-Promoting Surface Treatment
  • Light, Even Application by Wiping, Dipping
  • Room-Temperature Adhesive Cure

Product Description

DOWSIL™ PR-1204 RTV Prime Coat is a clear liquid adhesion promoter used before moisture-cure RTV or heat-cure silicone application. Applied as a very light, even film, it improves silicone bonding to many metals, glass, ceramics and masonry. The product can be wiped, dipped or sprayed, with typical non-volatile content of 7.9% and 180-degree peel strength of 66 ppi (45.5 N/cm²) on aluminum. After application, the carrier solvent evaporates and the active ingredients cure with atmospheric moisture, typically for 1 to 2 hours at room temperature and 20 to 90% relative humidity. Surface cleanliness, thin-film control and complete primer cure are important to bonding performance.

Key features

  • Multi-substrate adhesion promotion: Supports RTV and heat-cure silicone bonding to many metals, glass, ceramics and masonry.
  • Flexible application methods: Applies by wiping, dipping or spraying as a very light, even coat.
  • Room-temperature moisture cure: Typically cures for 1 to 2 hours at 20 to 90% relative humidity.
  • Aluminum peel result: Typical 180-degree peel strength is 66 ppi (45.5 N/cm²) on aluminum.
  • Defined storage life: Typical shelf life is 18 months at 25°C when stored and handled as directed.

Suitable for

  • Moisture-cure RTV silicone bonding processes.
  • Heat-cure silicone bonding processes.
  • PCB system assemblies requiring evaluation of primer-assisted silicone adhesion.

Technical Specifications

No specifications available.

Additional Information

Surface Treatments | Adhesion Primers and Promoters

DOWSIL™ PR-1204 RTV Prime Coat

DOWSIL™ PR-1204 RTV Prime Coat is a clear adhesion-promoting surface treatment for moisture-cure RTV and heat-cure silicone systems. Applied as a very thin film, it supports bonding to many metals, glass, ceramics and masonry. Typical data include 7.9% non-volatile content and 180-degree peel strength of 66 ppi (45.5 N/cm²) on aluminum; these values are not specifications.

Clear liquid primer 7.9% non-volatile content Wipe, dip or spray 1-2 hour room-temperature cure 66 ppi peel on aluminum 18-month shelf life at 25°C

DOWSIL PR-1204 RTV Prime Coat.

As supplied

Typical as-supplied properties

Values are typical and should not be used as product specifications.

Property Value Unit Method / condition
Physical state Liquid - As supplied
Color Colorless to pale yellow - As supplied
Non-volatile content 7.9 % Typical value
Kinematic viscosity 1 mm²/s At 25°C
Relative density 0.77 - Water = 1
Processing

Application process

Bonding performance depends on surface preparation, complete wetting, very light primer application and full primer cure before the silicone elastomer is applied.

Surface preparation: Use mild abrasion when practical, then clean or degrease the surface with a suitable solvent. A final acetone or IPA wipe may be helpful. Allow cleaning solvents to evaporate completely before priming.
Application: Apply a very light, even coat by wiping, dipping or spraying. For wipe application, add fresh cleaner or primer to the cloth every 3 to 5 minutes.
Film control: Wipe off excess material to avoid overapplication. For dip or spray coating, dilution by a factor of 2 to 4 with additional solvent may reduce excessive build-up.
Cure before bonding: Cure at room temperature for 1 to 2 hours at 20 to 90% relative humidity. Low temperature or humidity requires more time. Mild heat may accelerate cure, but temperatures above 60°C (140°F) are not recommended. Apply the silicone after the primer is fully cured.
Storage and Handling

Store below 32°C (90°F), keep containers tightly closed, minimize headspace and prevent moisture ingress. Partially filled containers may be purged with dry air or nitrogen. Pour only small amounts for immediate use into clean, dry containers and discard remaining material after use. Do not use material that becomes milky or contains a large amount of white precipitate. Typical shelf life is 18 months at 25°C. The product is highly flammable; keep it away from heat, sparks, flames and other ignition sources, and use appropriate ventilation and protective measures in accordance with the current regional SDS.

Application control guidance

Issue or observation Technical guidance Qualification boundary
White or chalky surface after application This generally indicates overapplication. Wipe off excess material and reduce the applied coat. For dip or spray processes, 2- to 4-fold dilution with additional solvent may help limit build-up. Confirm the selected dilution and application process by testing with the actual substrate and silicone system.
Cure is slower than expected Low temperature or humidity extends cure time. Allow additional time. Mild heat may accelerate cure, but temperatures above 60°C (140°F) are not recommended. Determine the appropriate cure schedule for the actual temperature, humidity, substrate and assembly conditions.
Milky appearance or substantial white precipitate These conditions indicate moisture contamination. Do not use the affected material. A small amount of white precipitate limited to the container-cap area does not affect the bulk material.
Poor wetting or inconsistent adhesion Review surface cleanliness and reactivity. Mild abrasion, solvent cleaning and, for difficult surfaces, chemical or energy-based pretreatment may improve surface preparation. Select and validate the preparation method for the exact substrate, finish, contamination state and silicone system.
Use contexts

Applications

The primer is relevant where a thin adhesion-promoting treatment is required before applying compatible RTV or heat-cure silicone to a prepared surface. Validate the complete substrate, primer, silicone and cure combination for the intended assembly.

Moisture-cure RTV silicone bonding
Use as a light primer coat before applying compatible moisture-cure RTV silicone to prepared metals, glass, ceramics or masonry. Allow the primer to cure completely before silicone application.
Heat-cure silicone bonding
Use where adhesion promotion is required between a compatible heat-cure silicone and a supported prepared substrate. Confirm surface preparation, primer cure and the complete silicone cure process by application testing.
PCB system assemblies
Evaluate as an adhesion-promoting treatment in PCB system assemblies where a silicone elastomer must bond to a selected substrate. Verify material compatibility, process temperature and assembly-level performance in the intended design.
Next steps

Evaluate DOWSIL PR-1204 for your silicone bonding process

Krayden can help review substrate preparation, application method, primer film control, cure conditions and silicone compatibility for your assembly. Share your substrate, process and performance requirements to plan product evaluation and confirm an appropriate handling and test approach.