DOWSIL ME-4131

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

DOWSIL ME-4131

Main features

  • One-Part Clear Addition-Cure Silicone Coating for Die Coating
  • 6,575 cP Application Viscosity
  • 19 kV/mm Dielectric Strength

Product Description

DOWSIL™ ME-4131 Encapsulant Clear is a one-part, clear addition-cure silicone elastomer coating for die coating and wire-bond packaging. The ready-to-use microelectronics-grade material requires no mixing and is documented for manual or automated dispensing. Typical as-supplied viscosity is 6,575 cP, with a heat-cure condition of 120 minutes at 150°C and nine-month shelf life under cold storage. After cure, the material provides low modulus, optical clarity, electrical insulation, controlled ionic impurities, and stress absorption for microelectronic and discrete-device protection.

Key features

  • Ready-to-use one-part coating: The clear addition-cure silicone requires no mixing.
  • Microelectronics-grade purity: Typical ionic impurity data include 0.2 ppm Na+, 0.4 ppm K+, and 2.1 ppm Cl-.
  • Electrical and optical properties: Typical cured data include 19 kV/mm dielectric strength and a 1.41 refractive index.

Applications / Suitable for

  • Die coating for wire-bond packaging
  • Microelectronic device protection
  • Discrete-device and optical packaging

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or mixed-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Product form One-part silicone coating N/A As supplied
Color Clear N/A As supplied
Viscosity 6,575 cP Typical
Specific gravity 1.04 N/A Typical
Shelf life 9 months At -25°C to -10°C
Heat-cure condition 120 min At 150°C
Technical properties

After-processing / final-state properties

Typical final-state values under the stated system and test conditions. These values are not sales specifications.

Property Value Unit Method / condition
Hardness 31 Shore A Typical cured value
Refractive index 1.41 N/A Typical cured value
Dielectric strength 19 kV/mm Typical cured value
Volume resistivity 1.4 × 10¹⁵ ohm·cm Typical cured value
Linear coefficient of thermal expansion 350 ppm/°C TMA
Sodium impurity 0.2 ppm Na+
Potassium impurity 0.4 ppm K+
Chloride impurity 2.1 ppm Cl-

Leading Brands Trust in Our Products and Services