DOWSIL 1-2620LV

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

DOWSIL 1-2620LV

Main features

  • Low-Viscosity Narrow-Gap Coating
  • Room-Temperature Moisture Cure
  • UV-Aided Automated Inspection

Product Description

DOWSIL 1-2620 Low VOC Conformal Coating is a one-part, translucent, low-viscosity silicone resin solution for protecting rigid and flexible circuit boards. The 350 mPa s coating flows into narrow gaps and spaces and can be applied by spray, brush, flow, dip, or automated pattern coating. It cures with atmospheric moisture at room temperature to a firm, elastoplastic, abrasion-resistant surface; mild heat can reduce tack-free time after adequate solvent flash-off. A UV indicator supports automated inspection. The product is intended for PCB applications that require toughness and abrasion resistance.

Key features

  • Low-viscosity gap coverage: The 350 mPa s coating flows into narrow gaps and spaces on PCB assemblies.
  • Room-temperature moisture cure: The coating cures without an oven, with optional mild heat acceleration after solvent flash-off.
  • UV-aided inspection: A UV indicator supports automated inspection of applied coating.

Applications / Suitable for

  • Protective coating for rigid circuit boards
  • Protective coating for flexible circuit boards
  • PCB system applications requiring toughness and abrasion resistance

Technical Specifications

General Properties
Color Color
Translucent (Clear)
Component System Component System
One
Specific Gravity Specific Gravity
1.12
Physical Properties
Viscosity Viscosity
350 mPa.s
Electrical Properties
Volume Resistivity Volume Resistivity
1.05E15 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical uncured and tack-free properties; heat-accelerated values require adequate solvent flash-off.

Property Value Unit Method / condition
Viscosity 350 mPa s Typical uncured property
Specific gravity 0.88 Uncured
Tack-free time 15 min 25 deg C
Heat-accelerated tack-free time 5 min 60 deg C and 15% RH
Typical cure schedule 10 min room temperature + 10 min at 60 deg C 3 mil (75 um) coating; after solvent flash-off
Technical properties

After-processing / final-state properties

Typical cured coating properties; electrical values apply to the cured material.

Property Value Unit Method / condition
Cured color Translucent, clear Cured coating
Specific gravity 1.12 Cured
Durometer 80 Shore A Cured coating
Dielectric strength 400 (16) V/mil (kV/mm) Cured coating
Volume resistivity 1.05 x 10^15 ohm cm Cured coating
Dielectric constant 2.49 100 Hz
Dielectric constant 2.48 100 kHz
Dissipation factor 0.002 100 Hz

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers