DK52 Gray Insulating Coating Powder

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

DK15-2000E Flexible Insulating Coating Powder for High Voltage Fuses and Low Voltage Busbars DK52 Gray Insulating Coating Powder Highest dielectric strength busbar coating Coating for high voltage fuses and axial leaded fuses Niche high voltage application - lightning arrestors Gray Busbar coating for low voltage busbars

Main features

  • DK52 Coating Powder
  • Gray, insulating, epoxy based
  • For high voltage fuses and low voltage bus bars

Product Description

A uniquely flexible insulating coating powder for high voltage fuses, lightning arrestors, low voltage busbars and other niche applications

DK52 Gray is a flexible, moisture-resistant epoxy coating powder developed for the insulation of high-voltage fuses, axial leaded fuses, and other high-voltage electrical apparatus. It offers very high flexibility, which provides maximum efficiency of low voltage busbar designs, which can often involve complex shapes. Besides being very flexible, DK52 Gray carries a UL recognition (RTI) for 100,000 hours at 105°C making it ideal for applications requiring high thermal stability. The fusion bonded coating is smooth, tough, and moisture-resistant for applications up to 600V. DK52 Gray is UL recognized.

Advantages of DK52 Gray for High Voltage Fuses and Other Niche Applications

  • Very flexible epoxy coating powder
  • High-voltage fuses and low-voltage busbars
  • Very high dielectric strength
  • Meets minimum RTI rating

Typical applications and uses include:

  • Low Voltage (600V) Copper, Aluminum and Brass Busbars
  • High Voltage Fuse Coating
  • Leaded Axial Fuse Coating
  • Lighting Arrestors
  • Switchgear Equipment for Power Distribution
Product Family

DK1008

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

{tab=Pricing & Availability}

Pricing for {product_name}

Pricing and Volume Price Breaks for {product_name} are available by contacting us. You cannot order this product directly online.

KRAYDEN lists all its prices without taxes, shipping payment charges or discounts. KRAYDEN has warehouses and ships from both Canada and the Netherlands, and if your shipping address is one of these two countries, applicable taxes will be applied. If your shipping address is to the United States, we request your company’s Employer Identification Number (EIN) or Tax Identification Number (TIN). This is a unique 9-digit number assigned by the IRS and is required for all cross-border shipments. Failure to provide this number could result in delays to your order. If your shipping address is within the EU, but outside the Netherlands, then we are required to request your company's Value Added Tax (VAT, BTW, MwSt) number to be able to ship the goods tax-free. For all other countries, no taxes are levied on your orders.

Minimum Order Quantity for {product_name}

The minimum order quantity for this package size is {min_order_quantity} {product_unit}(s).

Shipping Charges for {product_name}

All prices shown are ex-works KRAYDEN, but during the checkout process, you will be given several shipping options including Canada Post, TNT, UPS or the choice of using your own freight forwarder. Depending on your shipping address, the shipping charges will be calculated as follows:

  • Europe, Middle East, Asia and Africa: Shipping from KRAYDEN Europe BV (Amsterdam, the Netherlands)
  • Canada, USA, Mexico and South America: Shipping from KRAYDEN Corporation (Ottawa, Canada)

 


Payment option for {product_name}

During the checkout process, you will be presented with several payment options including:

  • Credit Card (We accept VISA and Mastercard)
  • Bank Transfer (You will be given the payment instructions at the time of order placement)
  • PayPal (Where you can also pay with American Express Cards)
  • Purchase Order (You must be preapproved first. See our Online Credit Application)

 

Availability for {product_name}

To the right of the product is a small icon that lets you know the availability and leadtime of the product. This leadtime is the time to ship the product and delivery times vary based on the method of delivery you select at the time you place your order. Contact us if anything is unclear or you need more assistance.

{tab=Technical Specifications}

Short Description of {product_name}

Technical Datasheets for {product_name}

TDS (English) Kapton_Technical_Data_Sheet Click to access {product_name} Technical Data Sheet
*Note that only registered users may access technical datasheets

{tab=Competitive Crossovers} #shortdesc

Compare price and quality of DK15-0907 Red Insulating Epoxy Coating Powder to these other brands

Please see the section above for a list of Competitive Brands that {product_name} competes against.

{tab=Videos & Other Media}

Videos & Other Related Media

Please visit or subscribe to our YouTube Channel.

See this video that shows the difference between a good and a bad fluidized epoxy coating powder bed.

{tab=Product Reviews}

Product Reviews for {product_name}

{review}

{tab=Packaging Details}

Packaging Details for {product_name}

The following information is specifically related to each unit of measure of {product_name}. If you which to compare this to other product sizes, click on the respective product from the list above and check here for values specific to that product. These values are taken from our internal database and are used in the calculation of the gross weight and packaging dimensions of the goods during shipping. You can use these values to to approximate delivery charges using your own carrier.

Each unit of {product_name} has the following:

  • Unit of Measurement: {product_unit}
  • Dimensions (length x width x height): {length} x {width} x {height} {lwh_uom}
  • Weight: {weight} {weight_uom}

 

{tab=View Blogs & Forum}

Read and discuss {product_name} on KRAYDEN's Blog and Forum
KRAYDEN is different. Unlike other business to business enterprises, we encourage our customers to discuss, critique, and otherwise comment on the products we offer. Get more technical information, read detailed posts, and see what customers have to say about about {product_name} on our Corporate Blog and Forum.

 

  • Read more about {product_name} on our Blog.
  • Join the discussion about {product_name} on our Forum.

{/tabs}

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers