COOLTHERM SC-6731

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

COOLTHERM SC-6731

Main features

  • 100 cP Resin Viscosity
  • Concentrations from 0.1% to 5% by Weight
  • Two-Component RTV Silicone Systems Used in Potting

Product Description

CoolTherm™ SC-6731 Hardener is a low-viscosity curing agent for use with compatible CoolTherm™ and Circalok™ silicone resins to form two-component, room-temperature-vulcanizing silicone systems for potting and encapsulation. The light amber, translucent liquid has a typical viscosity of 100 cP at 25°C and may be used at concentrations from 0.1% to 5% by weight, depending on the selected resin and required cure rate. Product-specific mixing ratios, working times, and cure schedules must be taken from the applicable silicone resin datasheet.

Key features

  • Low viscosity: Provides a typical viscosity of 100 cP at 25°C for incorporation into compatible silicone resin systems.
  • Adjustable concentration: May be used at 0.1% to 5% by weight, depending on the cure rate required and the applicable resin formulation.
  • Silicone-system versatility: Designed for use with various CoolTherm and Circalok silicone resins used in RTV potting and encapsulation systems.

Applications / Suitable for

  • Compatible CoolTherm and Circalok RTV silicone resin systems
  • Two-component silicone potting and encapsulation systems

Technical Specifications

General Properties
Appearance Appearance
Light Amber Translucent Liq
Specific Gravity Specific Gravity
1.1
Physical Properties
Viscosity Viscosity
100 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied properties and documented use concentration for CoolTherm SC-6731 Hardener. Values are not intended for specification purposes.

Property Value Unit Method / condition
Appearance Light amber, translucent liquid — As supplied
Viscosity 100 cP At 25°C; test method not stated
Specific gravity 1.1 — Test conditions and method not stated
Use concentration 0.1–5 wt% Depending on required cure rate; use the applicable resin datasheet for the specific mix ratio
Shelf life 6 months From date of manufacture when stored at 25°C in the original, unopened container