COOLTHERM SC-6705

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

COOLTHERM SC-6705

Main features

  • 55 to 205 deg C Service Range
  • 2,500 cP Mixed Viscosity
  • 17.7 kV/mm Dielectric Strength

Product Description

CoolTherm® SC-6705 Silicone Encapsulant is a two-component, addition-cure silicone system designed for applications requiring flexible encapsulation and high-temperature service. The resin and hardener mix at a 1:1 ratio by weight or volume to form a black liquid with a typical mixed viscosity of 2,500 cP at 25°C. After cure, the material forms a flexible elastomer with a documented operating-temperature range of -55°C to +205°C, typical thermal conductivity of 0.35 W/m·K, and electrical insulating properties.

Key features

  • Broad operating-temperature range: Suitable for parts and devices operating from -55°C to +205°C.
  • Low mixed viscosity: Provides a typical mixed viscosity of 2,500 cP at 25°C for encapsulation processing.
  • Flexible electrical insulation: The cured system provides 100% elongation at break, typical dielectric strength of 17.7 kV/mm, and volume resistivity of 1 × 1014 ohm-cm at 25°C.

Applications / Suitable for

  • Flexible silicone encapsulation requiring high-temperature service

Technical Specifications

General Properties
Appearance Appearance
Resin: Black Liq | Hardener: Off white Liq | Mixed: Black Liq
Specific Gravity Specific Gravity
1.35
Physical Properties
Viscosity (Part A) Viscosity (Part A)
(Resin) 3000 mPa.s
Viscosity (Part B) Viscosity (Part B)
(Hardener) 2900 mPa.s
Thermal Properties
Thermal Conductivity Thermal Conductivity
0.35 W/m.K
Mechanical Properties
Elongation Elongation
at break 100 %
Electrical Properties
Dielectric Strength Dielectric Strength
17.7 kV/mm
Volume Resistivity Volume Resistivity
1 x 10^14 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of CoolTherm SC-6705 resin, hardener, and mixed encapsulant before cure. Values are not intended for specification purposes.

Property Value Unit Method / condition
Appearance Black liquid / Off-white liquid / Black liquid — Resin / hardener / mixed system
Viscosity 3,000 / 2,900 / 2,500 cP Resin / hardener / mixed system at 25°C; test method not stated
Specific gravity 1.35 / 1.35 / 1.35 — Resin / hardener / mixed system; test conditions not stated
Mix ratio 1:1 Resin:hardener By weight or volume
Working life 1–2 hours Mixed system at 25°C; endpoint definition and test method not stated
Cure schedule 2 hours / 24 hours — At 65°C / room temperature; time begins after the material reaches the target temperature
Shelf life 6 months Each component when stored at 25°C in the original, unopened container
Technical properties

After-processing / final-state properties

Typical cured properties of CoolTherm SC-6705 Silicone Encapsulant. The source does not state the cure schedule used to prepare the cured-property specimens. Values are not intended for specification purposes.

Property Value Unit Method / condition
Operating temperature range -55 to +205 °C Documented range for parts and devices; retained-property data are not stated
Thermal conductivity 0.35 W/m·K Test method and temperature not stated
Hardness 60 Shore A Test method not stated
Tensile strength 2.07 (300) MPa (psi) Test method and test temperature not stated
Elongation at break 100 % Test method and test temperature not stated
Volume resistivity 1 × 1014 ohm-cm At 25°C; ASTM D257
Dielectric strength 17.7 (450) kV/mm (V/mil) ASTM D149; specimen thickness not stated
Dielectric constant 3.2 — At 100 Hz; ASTM D150
Dissipation factor 0.005 — At 100 Hz; ASTM D150

Leading Brands Trust in Our Products and Services