COOLTHERM SC-104

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

COOLTHERM SC-104

Main features

  • 0.8 W/(m K) Thermal Encapsulation
  • 7,000 cP Mixed Viscosity
  • 17.3 kV/mm Dielectric Strength

Product Description

CoolTherm® SC-104 Thermally Conductive Silicone Encapsulant is a two-component, addition-curing polydimethylsiloxane system for electrical and electronic encapsulation. The resin and hardener mix at a 1:1 ratio by weight or volume to form a gray liquid with a typical viscosity of 7,000 cP at 25°C. The material may be cured at room temperature or with heat and develops a flexible silicone elastomer with typical thermal conductivity of 0.8 W/m·K, dielectric strength of 17.3 kV/mm, and resistance to thermal shock.

Key features

  • Thermally conductive encapsulation: Provides typical cured thermal conductivity of 0.8 W/m·K using the Hot Disc Transient Method.
  • Low-stress silicone cure: Exhibits low shrinkage and stress on components while providing documented thermal-shock resistance.
  • Processing flexibility: Supports a 1:1 mix ratio by weight or volume and room-temperature or accelerated heat-cure schedules.

Applications / Suitable for

  • Electrical and electronic encapsulation
  • Encapsulation applications requiring thermal conductivity and electrical insulation

Technical Specifications

General Properties
Appearance Appearance
Resin: White Liq | Hardener: Black Liq | Mixed: Gray Liq
Specific Gravity Specific Gravity
2.10
Physical Properties
Viscosity (Part A) Viscosity (Part A)
6000 mPa.s
Viscosity (Part B) Viscosity (Part B)
6000 mPa.s
Thermal Properties
Thermal Conductivity Thermal Conductivity
0.8 W/m.K
Mechanical Properties
Elongation Elongation
at break 45 %
Chemical Properties
Moisture absorption Moisture absorption
0.10 %
Electrical Properties
Dielectric Strength Dielectric Strength
17.3 kV/mm
Volume Resistivity Volume Resistivity
2.2 x 10^15 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of CoolTherm SC-104 resin, hardener, and mixed encapsulant before cure. Values are not intended for specification purposes.

Property Value Unit Method / condition
Appearance White liquid / Black liquid / Gray liquid — Resin / hardener / mixed system
Viscosity 6,000 / 6,000 / 7,000 cP Resin / hardener / mixed system at 25°C; test method not stated
Specific gravity 2.10 / 2.10 / 2.10 — Resin / hardener / mixed system; test conditions not stated
Mix ratio 1:1 Resin:hardener By weight or volume
Gel time 60 minutes Mixed system at 25°C; test method not stated
Working life 50 minutes Mixed system at 25°C; test method not stated
Cure schedule 24 hours / 25–30 minutes / 10–15 minutes — At 25°C / 70°C / 100°C; time begins after the material reaches the target temperature
Shelf life 9 months Each component from date of manufacture when stored at 25°C in the original, unopened container
Technical properties

After-processing / final-state properties

Typical cured properties of CoolTherm SC-104. Values were measured after curing for 16 hours at 25°C followed by 2 hours at 100°C and are not intended for specification purposes.

Property Value Unit Method / condition
Thermal conductivity 0.8 W/m·K Hot Disc Transient Method
Coefficient of linear thermal expansion 160 ppm/°C ASTM C864; temperature region not stated
Hardness 65 Shore A ASTM D2240
Tensile strength 480 psi ASTM D412
Elongation at break 120 % ASTM D412
Moisture absorption 0.1 % ASTM D570-81
Volume resistivity 2.2 × 1015 ohm-cm ASTM D257 at 25°C
Dielectric strength 17.3 (440) kV/mm (V/mil) ASTM D149
Dielectric constant 3.06 — At 25°C and 1 MHz; ASTM D150
Dissipation factor 0.0075 — At 25°C and 1 MHz; ASTM D150

Leading Brands Trust in Our Products and Services