COOLTHERM EP-6008

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

COOLTHERM EP-6008

Main features

  • 8,000 cP Resin Viscosity
  • 1-Hour Working Window
  • 0.3 W/(m K) Thermal Interface

Product Description

CoolTherm® EP-6008 BLK Epoxy Resin is a black, filled epoxy resin formulated for use with compatible CoolTherm® or Thermoset™ hardeners to create two-component potting and encapsulation systems. The material is designed to flow around intricate and densely packaged circuitry while forming a rigid, electrically insulating cured compound. When combined with CoolTherm EP-6010 Hardener, the system provides a typical cured thermal conductivity of 0.3 W/m·K, a working life of 1 hour at 25 °C, and documented operating-temperature capability from -55 to 155 °C.

Key features

  • General-purpose encapsulation: Forms a two-component epoxy compound for potting and encapsulating intricate or densely packaged circuitry.
  • Low-viscosity resin: The resin has a typical viscosity of 8,000 cP at 25 °C to support flow around electronic components.
  • Electrical and thermal performance: The cured EP-6008 BLK/EP-6010 system provides typical thermal conductivity of 0.3 W/m·K and dielectric strength of 17.7 kV/mm.

Applications / Suitable for

  • General-purpose electronic potting and encapsulation
  • Intricate and densely packaged circuitry
  • Electrical assemblies requiring rigid, electrically insulating encapsulation

Technical Specifications

General Properties
Appearance Appearance
Black Liquid
Specific Gravity Specific Gravity
1.55
Physical Properties
Viscosity Viscosity
8000 mPa.s
Thermal Properties
Thermal Conductivity Thermal Conductivity
0.3 W/m.K
Mechanical Properties
Elongation Elongation
at break 1.8 %
Chemical Properties
Moisture absorption Moisture absorption
10 days @25°C 0.35 %
Electrical Properties
Dielectric Strength Dielectric Strength
17.7 kV/mm
Volume Resistivity Volume Resistivity
>10^14 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of CoolTherm EP-6008 BLK resin and the EP-6008 BLK/EP-6010 mixed system before cure. Values are not intended for specification purposes.

Property Value Unit Method / condition
Appearance Black liquid — CoolTherm EP-6008 BLK resin as supplied
Viscosity 8,000 cP Resin at 25 °C; test method not stated
Specific gravity 1.55 — Resin at 25 °C
Working life 1 hour EP-6008 BLK/EP-6010 mixed system at 25 °C
Cure time 12 or 2 hours EP-6008 BLK/EP-6010 system: 12 hours at 25 °C or 2 hours at 65 °C
Shelf life 1 year EP-6008 BLK resin stored at 25 °C in the original, unopened container
Technical properties

After-processing / final-state properties

Typical cured properties of the CoolTherm EP-6008 BLK/EP-6010 epoxy system. Values are not intended for specification purposes.

Property Value Unit Method / condition
Thermal conductivity 0.3 W/m·K EP-6008 BLK/EP-6010 cured system; test method not stated
Operating temperature range -55 to 155 °C Documented system operating range; retained individual properties are not stated
Hardness 85 Shore D EP-6008 BLK/EP-6010 cured system; test method not stated
Dielectric strength 17.7 (450) kV/mm (V/mil) EP-6008 BLK/EP-6010 cured system; specimen thickness and test method not stated