CONATHANE TU-401

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

CONATHANE TU-401

Main features

  • Two-Component Urethane Potting Prepolymer
  • Circuit-Board and Cable Encapsulation
  • Low-Viscosity High-Elongation Elastomer Systems

Product Description

CONATHANE® TU-401 Urethane Prepolymer is the amber Part A urethane prepolymer used in compatible two-component CONATHANE polyurethane casting and potting systems. When paired with the specified curative, the system is used for molding and potting electrical assemblies exposed to severe thermal changes. Documented applications include printed circuit boards, electrical cables, connectors, strain-sensitive devices, and wire-wound components. The associated polyurethane systems are described as having low viscosity, high elongation, hydrolytic stability, dielectric properties, and resistance to fungus and thermal shock.

Key features

  • Part A urethane prepolymer: TU-401 is the resin component of a compatible two-component polyurethane system.
  • Electrical assembly potting: Documented system uses include circuit boards, cables, connectors, and wire-wound devices.
  • Flexible elastomer systems: Compatible systems are documented for high elongation, hydrolytic stability, and thermal-shock resistance.

Applications / Suitable for

  • Resin component for polyurethane potting and molding
  • Printed circuit boards, cables, and connectors
  • Strain-sensitive and wire-wound electrical devices
Product Family

CONATHANE TU-401

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or mixed-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Component role Part A urethane prepolymer N/A As supplied
Color Amber N/A As supplied
Material form Liquid N/A As supplied
System type Two-component polyurethane N/A Requires compatible Part B curative