Main features

  • Low-Viscosity Silicone Mold Release
  • Epoxy/Polyurethane/Polyester/Plastic Resin Release
  • 10 to 15-Minute Air Dry

Product Description

CONAP® MR-5002 Mold Release is a low-viscosity, silicone-based liquid mold release and parting agent for casting, potting, and molding operations. The clear material forms a thin release film that supports reproduction of fine mold detail and is applied by dip, brush, spray, or slosh. It is documented for releasing epoxy, polyurethane, polyester, and many plastic resins from metal, plastic, and other nonporous molds. The product may be used with room-temperature or heat-curing systems and typically air dries in 10 to 15 minutes before casting.

Key features

  • Low-viscosity release film: Typical viscosity is 20 cP at 25°C.
  • Broad resin compatibility: The release agent is documented for epoxy, polyurethane, polyester, and many plastic resins.
  • Multiple application methods: It may be applied by dip, brush, spray, or slosh to clean nonporous molds.

Applications / Suitable for

  • Simple and complex casting molds
  • Potting and molding operations using nonporous tooling
  • Epoxy, polyurethane, polyester, and plastic-resin release
Product Family

CONATHANE MR-5002

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or mixed-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Product form Liquid mold release N/A As supplied
Color Clear N/A As supplied
Viscosity 20 cP At 25°C
Specific gravity 0.67 to 0.68 N/A At 25°C
Solids content 2.7 to 3.3 % Typical
Air-dry time 10 to 15 min Typical before casting
Optional heat drying 5 min At 60°C
Shelf life Indefinite N/A Legacy technical data