CONATHANE EN-12

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

CONATHANE EN-12

Main features

  • Flexible Two-Component Polyurethane System for Electrical
  • 6,500 cP Mixed Viscosity
  • Shore A 50 Hardness

Product Description

CONATHANE® EN-12 Polyurethane Encapsulant is a two-component, highly flexible polyurethane molding and encapsulation system using EN-4 Part A with EN-12 Part B. The translucent amber system is documented for cable and connector potting, electronic modules, wire-wound devices, strain-sensitive components, and thick-film protection of printed circuitry. It combines low dielectric constant, hydrolytic stability, thermal-shock resistance, and high dielectric strength across a recommended operating range of -65°C to 130°C. Typical initial mixed viscosity is 6,500 cP at 25°C with a 100:95 mix ratio by weight.

Key features

  • Highly flexible polyurethane: Typical cured hardness is Shore A 50 with 350% elongation.
  • Controlled mixed viscosity: Typical initial mixed viscosity is 6,500 cP at 25°C.
  • Electrical and environmental properties: Typical dielectric strength is 600 V/mil with thermal-shock and hydrolytic-stability data.

Applications / Suitable for

  • Cable and connector potting and molding
  • Electronic modules and wire-wound devices
  • Strain-sensitive components and printed circuitry

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or processing-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Part A viscosity 8,500 cP EN-4 Part A at 25°C
Part B viscosity 6,000 cP EN-12 Part B at 25°C
Part A specific gravity 0.97 N/A At 25°C
Part B specific gravity 0.91 N/A At 25°C
Mix ratio 100:95 parts by weight EN-4 Part A : EN-12 Part B
Initial mixed viscosity 6,500 cP At 25°C
Cure option 24 h At 60°C
Cure option 16 h At 80°C
Technical properties

After-processing / final-state properties

Typical cured or final-state values under the stated system and test conditions. These values are not sales specifications.

Property Value Unit Method / condition
Hardness 50 Shore A ASTM D2240
Tensile strength 400 psi ASTM D412
Ultimate elongation 350 % ASTM D412
Tear strength 75 pli ASTM D624
Dielectric strength 600 V/mil ASTM D149
Volume resistivity >4.3 × 10¹⁵ ohm·cm ASTM D257 at 25°C
Operating temperature -65 to 130 °C Recommended range