CONATHANE EN-11

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

CONATHANE EN-11

Main features

  • Flexible Two-Component Polyurethane System for Potting
  • 5,750 cP Mixed Viscosity
  • 350% Cured Elongation

Product Description

CONATHANE® EN-11 Polyurethane Encapsulant is a two-component, highly flexible polyurethane molding and encapsulation system for electrical and electronic assemblies exposed to severe environmental conditions. EN-4 Part A is mixed with EN-11 Part B at 100:55 by weight to produce a low-viscosity, translucent amber elastomer. The system is documented for cable and connector potting, electronic modules, wire-wound devices, strain-sensitive components, and thick-film protection of printed circuitry. Typical cured properties include Shore A 60 hardness, 350% elongation, high dielectric strength, hydrolytic stability, and thermal-shock resistance.

Key features

  • Flexible polyurethane system: The cured material has typical Shore A 60 hardness and 350% ultimate elongation.
  • Low mixed viscosity: Typical initial mixed viscosity is 5,750 cP at 25°C.
  • Electrical and environmental properties: Typical data include 610 V/mil dielectric strength, hydrolytic stability, and thermal-shock resistance.

Applications / Suitable for

  • Cable and connector potting and molding
  • Electronic module and wire-wound device encapsulation
  • Strain-sensitive component potting and printed-circuit protection

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or mixed-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Part A viscosity 8,500 cP EN-4 Part A at 25°C
Part B viscosity 4,000 cP EN-11 Part B at 25°C
Part A specific gravity 0.97 N/A At 25°C
Part B specific gravity 0.91 N/A At 25°C
Mix ratio 100:55 parts by weight EN-4 Part A : EN-11 Part B
Initial mixed viscosity 5,750 cP At 25°C
Cure options 24 h at 60°C; 16 h at 80°C N/A Recommended schedules
Shelf life 15 months Original unopened containers
Technical properties

After-processing / final-state properties

Typical final-state values under the stated system and test conditions. These values are not sales specifications.

Property Value Unit Method / condition
Hardness 60 Shore A ASTM D2240
Tensile strength 750 psi ASTM D412
Ultimate elongation 350 % ASTM D412
Tear strength 100 pli ASTM D624, Graves
Linear shrinkage 1.15 % Typical cured value
Dielectric strength 610 V/mil ASTM D149, 1/16 in specimen
Volume resistivity >4.3 × 10¹⁵ ohm·cm ASTM D257 at 25°C
Operating temperature range -65 to 130 °C Documented recommended range