CONATHANE CE-1170

Harmonization Code : 3404.90.00.00 | Artificial waxes and prepared waxes : Other

CONATHANE CE-1170

Main features

  • One-Component Acrylic Conformal Coating
  • 15-Minute Tack-Free Time
  • 2 x 10^15 ohm-cm Volume Resistivity

Product Description

CONAP® CE-1170 Acrylic Conformal Coating is a one-component, solvent-based acrylic conformal coating for printed circuit boards, epoxy-glass laminates, phenolic laminates, components, and other thin-film electronic applications. The coating is room-temperature or heat curable, with a typical tack-free time of 15 minutes, full cure in 24 hours at 25°C, or accelerated cure in 45 minutes at 60°C. It is documented as flexible, quick drying, repairable, humidity resistant, and hydrolytically stable, with a typical volume resistivity of 2 × 10¹⁵ ohm·cm.

Key features

  • One-component acrylic coating: The solvent-based material is used for thin-film protection of components and printed circuitry.
  • Fast handling: Typical tack-free time is 15 minutes, with room-temperature or accelerated heat cure.
  • Electrical insulation: Typical volume resistivity is 2 × 10¹⁵ ohm·cm.

Applications / Suitable for

  • Printed circuit boards and printed circuitry
  • Epoxy-glass and phenolic laminates
  • Thin-film coating of electronic components

Technical Specifications

Physical Properties
Viscosity Viscosity
400 mPa.s
General Properties
Appearance Appearance
Amber, slight haze
Specific Gravity Specific Gravity
0.95
Thermal Properties
Flash Point Flash Point
13 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or mixed-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Chemical base Acrylic N/A One-component solvent-based coating
Color Amber N/A One-gallon can configuration
Specific gravity 0.93 N/A As supplied
Viscosity 400 cP As supplied
Tack-free time 15 min Typical
Cure options 24 h at 25°C; 45 min at 60°C N/A Room-temperature or heat cure
Flash point 7 °C One-gallon can configuration