BONDERITE C-MC 5884

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

BONDERITE C-MC 5884

Main features

  • MIL-C-85704C Type I Qualification
  • GE and Pratt and Whitney Engine Listings
  • Ash-Free Water-Miscible Cleaning

Product Description

BONDERITE C-MC 5884 AERO is a concentrated liquid maintenance cleaner formulated to remove oil, salt, and solid deposits from the compressor blades, guide vanes, and rotors of in-service jet engines. Periodic cleaning with this product helps address the power loss, abnormal temperature rise, and increased fuel consumption that can result from compressor fouling. The cleaner meets MIL-C-85704C Type I and is listed in General Electric and Pratt and Whitney engine-cleaning specifications. It is ash-free, low in phenol, chloride, and sulfur, and readily miscible with water. It is diluted with distilled or demineralized water at ratios of 1 to 4 or 1 to 1 depending on the cleaning procedure, and it has a minimum flash point of 65 deg C (Tag Closed Cup).

Key features

  • MIL-C-85704C Type I Qualification: meets the requirements of and is approved to MIL-C-85704C Type I
  • GE and Pratt and Whitney Engine Listings: listed in General Electric SPM REF C04-140 and Pratt and Whitney SPMC-87
  • Ash-Free, Water-Miscible Formula: ash free, low in phenol, chloride, and sulfur, and readily miscible with water

Applications

In-service cleaning of jet-engine compressor blades, vanes, and rotors.

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
AppearanceClear liquidAs supplied
Density1.09 to 1.11g/mLAs supplied
pH4.21.5% dilution in DI water
Storage temperature0 to 40deg CRecommended storage range