BONDERITE C-IC 4104

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

BONDERITE C-IC 4104

Main features

  • Nitric Acid Descaling Enhancement
  • Multi-Alloy Pickling Compatibility
  • Alloy-Tailored Bath Formulation

Product Description

BONDERITE C-IC 4104 AERO is a clear, colorless liquid acidic additive blended into nitric acid and water solutions to enhance the descaling and pickling of stainless steels and heat-resistant alloys, including titanium, by immersion. It is also effective for descaling or pickling cobalt, chrome, nickel, and copper-based alloys. The additive readily mixes with nitric acid at recommended dilutions, and bath compositions can be tailored to the specific alloy being processed. As supplied, the product has a density of 1.09 to 1.11 g/mL and a pH of 4.2 at 1.5 percent dilution in deionized water, and it should be stored between 0 and 40 deg C.

Key features

  • Nitric Acid Bath Additive: added to nitric acid and water solutions to enhance descaling and pickling
  • Multi-Alloy Descaling and Pickling: effective on stainless steels, heat-resistant alloys, titanium, cobalt, chrome, nickel, and copper-based alloys
  • Alloy-Tailored Bath Formulation: solutions can be tailored to specific alloys and readily mix with nitric acid at recommended dilutions

Applications

Immersion descaling and pickling of stainless steel, heat-resistant alloys, and titanium in nitric-acid baths.

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
AppearanceAmber liquidAs supplied
DilutionUp to 15% v/vWith water, as-used bath
Immersion temperature80 to 95deg CProcess bath
Immersion time15 to 60minutesWith mechanical agitation
Tank materialStainless steelRequired equipment material