BONDERITE C-AK LS

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

BONDERITE C-AK LS

Main features

  • Rolling-Oil Steel-Strip Cleaning
  • Dip, Spray, or Electrolytic Cleaning
  • Oil-Separating Emulsion Behavior

Product Description

BONDERITE® C-AK 71110 (LS-TP1 (DE)) is a pale-yellow, clear, highly alkaline, heavy-duty industrial cleaner for steel-strip processing. Suitable for dip, spray, and electrolytic cleaning, it supports rapid removal of rolling oils before continuous annealing, electroplating, and galvanizing. Its surfactant blend promotes penetration and emulsification across a range of rolling oils, while the resulting emulsions are formulated to separate on standing for subsequent oil removal and effluent treatment.

Key features

  • Heavy-duty steel-strip cleaning: Formulated for fast, efficient removal of rolling oils before continuous annealing, electroplating, and galvanizing.
  • Flexible process application: Suitable for dip, spray, and electrolytic cleaning systems.
  • Oil-separating emulsion behavior: Allows emulsified oil to separate on standing for subsequent removal and effluent processing.

Applications / Suitable for

  • Cleaning steel strip before continuous annealing
  • Cleaning steel strip before electroplating
  • Cleaning steel strip before galvanizing
  • Dip-cleaning systems
  • Spray-cleaning systems
  • Electro-cleaning systems

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Supplier-published as-supplied characteristics and storage information for BONDERITE® C-AK 71110.

Property Value Unit Method / condition
Product type Alkaline industrial cleaner — Heavy-duty liquid cleaner for steel strip
Appearance Pale yellow, clear liquid — As supplied
Specific gravity 1.33 — At 20°C
Storage-temperature range 0 to 40 °C Supplier-published storage condition
Shelf life 24 months In unopened original packaging