BONDERITE C-AK ALUM

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

BONDERITE C-AK ALUM

Main features

  • Removal of Light Soils with Immersion Etching
  • Promotes Uniform Wetting Through Low Surface Tension
  • 40 to 80 deg C Service Range

Product Description

BONDERITE® C-AK ALUM ETCH 2L AERO is a slightly hazy alkaline cleaner etchant formulated to remove light soils and etch aluminum in immersion processes. Its low-surface-tension working solution promotes uniform wetting of aluminum surfaces and produces a smooth matte finish. The product is suitable for metal pretreatment of aluminum extrusions, structural shapes, aircraft components, truck bodies, and similar parts.

Key features

  • Combined cleaning and etching: Removes light soils while etching aluminum during immersion processing.
  • Uniform surface wetting: Low surface tension promotes even contact with the aluminum surface.
  • Smooth matte finish: Produces a uniform matte appearance on aluminum components.
  • Broad aluminum-part suitability: Supports pretreatment of extrusions, structural shapes, aircraft components, truck bodies, and similar parts.

Applications / Suitable for

  • Immersion cleaning and etching of aluminum
  • Aluminum extrusions
  • Aluminum structural shapes
  • Aircraft components
  • Truck bodies and similar aluminum parts
  • Metal pretreatment processes

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Supplier-published as-supplied characteristics and storage information for BONDERITE® C-AK ALUM ETCH 2L AERO.

Property Value Unit Method / condition
Technology Metal pretreatment — Supplier classification
Product type Alkaline cleaner etchant — Supplier classification
Application Immersion — Supplier classification
Appearance Slightly hazy liquid — As supplied
Storage temperature +5 to 50 °C Supplier-published storage range
Shelf life 24 months In unopened original packaging
Technical properties

After-processing / operating properties

Supplier-published operating conditions and process sequence for immersion cleaning and etching of aluminum.

Property Value Unit Method / condition
Working concentration 65–105 g/L Immersion-system solution make-up
Operating temperature 40–80 °C With mechanical agitation
Normal contact time 3–5 minutes Immersion process
Agitation Mechanical — Required during immersion processing
Post-etch rinse Cold to warm water — Rinse as soon as possible after cleaning
Subsequent treatment Deoxidize / desmut, rinse and dry — After initial water rinse
Resulting surface appearance Smooth matte finish — On aluminum surfaces under suitable process conditions

Leading Brands Trust in Our Products and Services