BONDERITE C-AK 319

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

BONDERITE C-AK 319

Main features

  • Spray-or-Immersion Application Flexibility
  • Effective Across Wide Concentration Range
  • Multi-Metal Pre-Plating Surface Prep

Product Description

BONDERITE C-AK 319 is a one-part, strongly alkaline liquid cleaner formulated to prepare aluminum, steel, electrogalvanized, and hot-dip galvanized surfaces for conversion coating or plating. Applied by spray or immersion, it operates over a wide concentration range and a temperature range of 120 to 180 deg F depending on substrate, with steel and galvanized surfaces run hotter than aluminum. Bath makeup is typically 1 to 6 gallons per 100 gallons of working volume. Process equipment may be constructed of mild steel, with 300 series stainless steel spray nozzles and PTFE seals recommended for contact components. The cleaner is intended for use ahead of BONDERITE conversion-coating processes.

Key features

  • Multi-Metal Compatibility: cleans aluminum, steel, electrogalvanized, and hot-dip galvanized steel surfaces
  • Spray or Immersion Processing: applied by either method at 120 to 180 deg F depending on substrate
  • Wide-Range Bath Concentration: effective over a wide concentration range with bath makeup of 1 to 6 gallons per 100 gallons

Applications

Cleaning aluminum, steel, electrogalvanized steel, and hot-dip galvanized steel before conversion coating or plating.

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Property Value Unit Method / condition
Operating temperature, aluminum120 to 140deg FImmersion or spray bath
Operating temperature, steel and galvanized140 to 180deg FImmersion or spray bath
Processing time, spray0.5 to 3minutesSpray application
Processing time, immersion0.5 to 6minutesImmersion application
Bath makeup1 to 6gal per 100 gal waterWorking bath concentration