BIOACT 105

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

BIOACT 105

Main features

  • High-Solvency Aerospace Soil Removal
  • Manual-Wipe or Immersion Cleaning
  • AMS 3167 Aerospace Conformance

Product Description

BIOACT 105 is a high-purity, fast-drying solvent cleaner for manual degreasing, damp-dry surface preparation, and room-temperature immersion cleaning. Its citrus-terpene, alcohol, and hydrocarbon blend combines a Kauri-Butanol value above 150 with low surface residue and a vapor pressure of 1.5 mmHg at 20°C. The cleaner removes adhesives, greases, corrosion inhibitors, paint overspray, silicones, waxes, and other industrial soils. It is compatible with many polymeric substrates and elastomers and can be used on ferrous and non-ferrous alloys. BIOACT 105 also conforms to AMS 3167 and is documented for multiple aerospace OEM cleaning processes.

Key features

  • High solvency: Kauri-Butanol value greater than 150.
  • Fast-drying, low-residue cleaning: Supports controlled manual and immersion cleaning.
  • Flexible application: Suitable for hand wiping, damp-dry surface preparation, and room-temperature immersion.
  • Broad soil-removal scope: Removes adhesives, greases, corrosion inhibitors, paint overspray, silicones, waxes, and other documented soils.
  • Material compatibility: Documented for many polymeric substrates and elastomers and for ferrous and non-ferrous alloys.
  • Aerospace process acceptance: Conforms to AMS 3167 and is documented for multiple aerospace OEM cleaning processes.

Applications / Suitable for

  • Manual cleaning and degreasing
  • Surface preparation before bonding, sealing, coating, or painting
  • Room-temperature immersion and soak-tank cleaning
  • Commercial and general aviation maintenance and precision cleaning
Product Family

BIOACT 105

Loading pricing…

Technical Specifications

No specifications available.

Additional Information

Surface Treatments | Solvent Cleaner

BIOACT 105

BIOACT 105 is a high-purity, fast-drying solvent cleaner for manual degreasing, damp-dry surface preparation, and room-temperature immersion cleaning. Its Kauri-Butanol value above 150 supports removal of difficult industrial soils, while low surface residue and compatibility with many alloys, polymers, and elastomers support controlled cleaning across aerospace and precision-manufacturing workflows.

High-purity solvent blend KB value >150 1.6 cP at 25°C 41°C flash point Manual or immersion use

Vantage Can

Product data

As-Supplied Properties

Typical product data for evaluation. These values are not guaranteed specifications.

Property Value Unit Method / condition
Appearance Clear liquid — As supplied
Odor Mild citrus/alcohol — As supplied
Flash point 41 (105) °C (°F) Closed cup
Specific gravity 0.80 — 25°C
Viscosity 1.6 cP 25°C
Vapor pressure 1.5 mmHg 20°C
Kauri-Butanol value >150 — Typical solvency value
Application

Application and Processing

Choose the cleaning method based on the substrate, soil, and downstream process. Confirm compatibility under actual use conditions before broad implementation.

Concentration: Use full strength for manual cleaning, damp-dry surface preparation, and immersion cleaning.
Manual application: Apply to the substrate with a brush, pad, or cloth.
Immersion: Add full-strength cleaner to the wash-tank reservoir; do not use heat or ultrasonics.

 

Application Sequence

Stage 1
Confirm substrate and cleaning task
Identify the substrate, contamination, and downstream bonding, sealing, coating, or painting requirements. Verify compatibility under actual use conditions.
Stage 2
Apply at full concentration
For manual cleaning, use a brush, pad, or cloth. For immersion cleaning, charge the wash tank with BIOACT 105 at full strength.
Stage 3
Complete the selected method
For damp-dry surface preparation, wipe the wetted surface with a clean, dry, low-lint towel before the solvent evaporates. For immersion cleaning, do not add heat or ultrasonics.
Storage and Handling

Store BIOACT 105 in its original, sealed container above 50°F (10°C). The documented shelf life is 36 months under these conditions. Keep the container tightly closed in a cool, well-ventilated storage area and consult the current SDS for complete safe-handling, fire-prevention, and disposal requirements.

Technical Guidance

Documented soils
Suitable cleaning targets include adhesives, inks, asphaltic residues, mold-release compounds, buffing and polishing compounds, corrosion inhibitors, coolants, fingerprints, greases, hydraulic fluids, paint overspray, particulate matter, sealants, silicones, tars, and waxes.
Substrate compatibility
The cleaner is documented for many polymeric substrates and elastomers and for ferrous and non-ferrous alloys. Validate the exact material, surface finish, exposure time, and downstream process under production conditions.

Approvals and Conformance

Issue or observation Source-supported guidance Qualification boundary
Aerospace general Conforms to AMS 3167. Confirm the current specification revision and customer or program requirements before use.
Boeing and Douglas Boeing D6-17487 Rev L, except ASTM F-484; BSS 7432; Douglas CSD #1. Apply only within the stated tests, exclusions, and process scope.
OEM process listings Bell Helicopter Bulletin 1915; Bombardier BAPS 180-009 General; CFM CP# 2719 Rev 76; GE Method 23 / C04-251 and listed alternatives; Gulfstream GAS115H; Honeywell C5049. Use the exact OEM document, part, substrate, and cleaning method required by the program.
Engine manufacturer requirements Pratt & Whitney SPOP 208, POP 1800-U, PMC 8929, and PWA 36604 Hot Corrosion; Rolls-Royce CSS No. 255 Type A and OMat 1/257S. Do not extend acceptance beyond the named process or material scope.
Airline use United Airlines SOL3001-17 and SOL3001-17WL10X12. Verify the correct product form and current airline process document.
ASTM testing ASTM F-945, F-1110, F-502, F-519, F-485, F-482, and F-2111. Test completion does not create universal substrate or process suitability.
Supported use contexts

Applications

BIOACT 105 supports full-strength manual and immersion cleaning where strong solvency, low surface residue, and controlled application are required.

Manual cleaning and degreasing
Apply full-strength cleaner by brush, pad, or cloth to remove oils, greases, adhesive residue, corrosion inhibitors, paint overspray, and other documented soils.
Damp-dry surface preparation
Use before bonding, sealing, coating, or painting. Wet the substrate with BIOACT 105, then wipe with a clean, dry, low-lint towel before the solvent evaporates.
Room-temperature immersion cleaning
Charge an immersion or soak tank with full-strength cleaner for batch component cleaning. The documented process does not recommend heat or ultrasonics.
Next steps

Technical Support

Work with Krayden to review BIOACT 105 against your substrate, soil, cleaning method, and aerospace process requirements. Our team can help evaluate material compatibility, application conditions, applicable specifications, packaging needs, and sample requirements before implementation.