AXAREL 6100

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

AXAREL 6100

Main features

  • Broad Multi-Soil Solvency
  • Hand-Wipe or Immersion Cleaning
  • 142 deg F Flash Point

Product Description

AXAREL 6100 Solvent Cleaner is a non-aqueous, aliphatic hydrocarbon precision cleaner formulated to combine low odor, minimal surface residue, and broad solvency. It is designed for hand-wipe and immersion cleaning at full concentration and can remove difficult soils including adhesives, inks, greases, hydraulic fluids, coolants, waxes, silicones, tars, paint overspray, and particulate matter. AXAREL 6100 offers a moderate drying rate, good soil loading, and material compatibility for cleaning and surface-preparation operations. It may be considered as an alternative to isopropyl alcohol, acetone, methyl ethyl ketone, and other lower-flash-point solvents, subject to process validation and applicable safety requirements.

Key features

  • Broad solvency: Removes a wide range of difficult industrial soils, including greases, oils, adhesives, inks, sealants, silicones, tars, waxes, and particulates.
  • Manual and immersion cleaning: Used at full concentration for hand wiping, immersion tanks, and compatible low-pressure spray-under-immersion systems.
  • Moderate drying rate: Provides more working time than faster-evaporating solvents while supporting practical room-temperature cleaning.
  • Low odor and low vapor pressure: Mild odor with vapor pressure below 1.0 mmHg at 20 °C.
  • Alternative to common low-flash-point solvents: May replace IPA, MEK, or acetone in suitable validated processes.

Applications / Suitable for

  • Manual precision cleaning and degreasing
  • Immersion and low-pressure spray-under-immersion cleaning
  • Surface preparation before subsequent manufacturing, coating, bonding, or inspection operations
Product Family

AXAREL 6100

Loading pricing…

Technical Specifications

No specifications available.

Additional Information

Surface Treatments | Precision Solvent Cleaner

AXAREL 6100 Solvent Cleaner

AXAREL 6100 is a non-aqueous aliphatic hydrocarbon precision cleaner developed for low odor, minimal surface residue, and broad solvency. It supports full-concentration hand-wipe and immersion cleaning for difficult industrial soils and may be evaluated as an alternative to IPA, MEK, acetone, and other lower-flash-point solvents.

Aliphatic hydrocarbon Mild odor 142 °F (61 °C) flash point Manual and immersion cleaning Broad solvency

As-supplied properties

Typical physical properties

Typical values are provided for product evaluation and are not guaranteed specifications unless explicitly identified as such.

Property Value Unit Condition / context
Product type Non-aqueous aliphatic hydrocarbon cleaner — As supplied
Odor Mild — Typical
Flash point 142 / 61 °F / °C Closed-cup value reported in product literature
Specific gravity 0.82 — 25 °C
Viscosity 1.6 cP Typical
Kauri-butanol value 39.6 — Typical solvency index
Vapor pressure <1.0 mmHg 20 °C
Processing

Full-concentration manual and immersion cleaning

AXAREL 6100 is used at full concentration. Select the cleaning method according to the soil, substrate, part geometry, cleanliness requirement, and equipment configuration. Validate compatibility and the required cleaning endpoint before production use.

Manual cleaning: Apply at full concentration to the desired substrate using a brush, pad, or cloth.
Immersion cleaning: Add at full concentration to the wash-tank reservoir.
Equipment: Suitable for compatible immersion tanks and low-pressure spray-under-immersion systems.
Process limitation: The product literature does not recommend the use of ultrasonics or heat.
Cleaning performance

Broad soil-removal capability

AXAREL 6100 is documented for removing a broad range of difficult process and maintenance soils. Actual cleaning performance depends on soil loading, dwell, agitation, substrate, part geometry, and bath condition.

Adhesives
Inks
Asphalts
Mold release compounds
Buffing compounds
Paint overspray
Corrosion inhibitors
Particulate matter
Coolants
Polishing compounds
Fingerprints
Sealants
Greases
Silicones
Tars
Hydraulic fluids
Waxes
Applications

Precision cleaning, degreasing, and surface preparation

The documented application scope includes aviation, commercial and general cleaning, and precision cleaning. Confirm the exact substrate, soil, downstream process, and approval requirements for each use.

Manual precision cleaning
Hand-wipe removal of difficult soils from components using a brush, pad, or cloth at full concentration.
Immersion degreasing
Cleaning in compatible immersion tanks or low-pressure spray-under-immersion equipment where good soil loading and moderate dry time are useful.
Surface preparation
Cleaning before subsequent processing, coating, bonding, assembly, inspection, machining, grinding, or polishing when validated for the specific process.
Approvals and testing

Documented aerospace references

Confirm the current document revision, exact product designation, application scope, and certification requirements before use.

Organization / test Documented reference
Bell Helicopter Bulletin No. 1915, Solvents, Blended Organic, Cold Degreasing
Goodrich Actuation Systems 981-100-020 Issue 4, Solvent Degreasing
Rolls-Royce CSS No. 255 Type A Non-Halogenated Organic Solvent Cleaner (MLC104)
Pratt & Whitney Hot corrosion testing of standard gas-turbine engine alloys (AMS 4037, 4375, 6359, 5508, 5536, 5544, 5608)
Testing SAE ARP 1755B; ASTM F945 at 20% and 100%
Storage and packaging

Original sealed container storage

The documented shelf life is 36 months when AXAREL 6100 is stored in its original, sealed container above 50 °F (10 °C). Documented package formats include 31 lb (14 kg) pails and 365 lb (166 kg) drums.

Keep containers closed and follow the current safety data sheet, site solvent-handling procedures, applicable fire controls, ventilation requirements, and local regulations for storage, use, and disposal.

Next steps

Evaluate AXAREL 6100 for your cleaning process

Krayden can help review soil type, substrate compatibility, cleaning equipment, drying requirements, downstream processes, and applicable aerospace specifications for AXAREL 6100.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers