ARALDITE TDR 1100-11

Harmonization Code : 8529.90 | Parts solely or principally used for TV, radio, and transmission

ARALDITE TDR 1100-11

Main features

  • Glass, Plastic, and Wood Bonding
  • 2:1 Meter-Mix Processing
  • 90-Minute Working Window

Product Description

TDR 1100-11 is a thixotropic, two-part epoxy adhesive specifically formulated for bonding glass laminate, wood, and plastic components. Designed primarily for use in the construction of archery bows, this system features a convenient 2:1 by volume mix ratio that is well-suited for automated metering equipment.

Key features

  • Extended working time: Features a long pot life of over 90 minutes to accommodate complex assembly processes.
  • Accelerated processing: Cures quickly at temperatures above 170°F (77°C) to help streamline production.
  • Aesthetic finish: Formulated to produce a clear bond line, preserving the visual quality of the final assembly.

Applications / Suitable for

  • Formulated for the construction of archery bows.
  • Bonding glass laminate components.
  • Bonding wood and plastic materials.
Product Family

ARALDITE TDR 1100-11

Loading pricing…

Technical Specifications

General Properties
Mix Ratio Mix Ratio
2:1
Pot Life Pot Life
95 minutes
Mechanical Properties
Elongation Elongation
3.6% to 4.6% (depending on cure schedule) %

Additional Information

Technical properties

As-supplied / before-processing properties

Pre-cure physical and processing characteristics of TDR 1100-11.

Property Value Unit Method / condition
Mix Ratio (Volume) 2:1 - Resin to Hardener
Mix Ratio (Weight) 100:42 - Resin to Hardener
Viscosity (Mixed System) 13,000 cP ASTM D2393
Pot Life 95 minutes 4 fl oz, ASTM D2471
Technical properties

After-processing / final-state properties

Cured mechanical properties of TDR 1100-11 when cured for 15 minutes at 180°F (82°C).

Property Value Unit Method / condition
Ultimate Strength 9,100 (62.7) psi (MPa) Cure: 15 min at 180°F (82°C)
Lap Shear Strength (at 77°F) 3,520 (24.3) psi (MPa) Cure: 15 min at 180°F (82°C)
Modulus of Elasticity 396,000 (2,731) psi (MPa) Cure: 15 min at 180°F (82°C)
Heat Deflection Temperature 164 (73) °F (°C) Cure: 15 min at 180°F (82°C)