ARALDITE MY721

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

ARALDITE MY721

Main features

  • Low-Viscosity Reinforcement Wet-Out
  • Long Processing Pot Life
  • High-Temperature Composite Performance

Product Description

ARALDITE MY 721 Epoxy Resin is a clear brown liquid tetrafunctional glycidylamine resin component for high-temperature composite systems. Typical viscosity is 3,000 to 6,000 cP at 50 deg C, with density of 1.15 to 1.18 g/cm^3 at 25 deg C, providing a low-viscosity processing profile for reinforcement wet-out. Used with ARADUR 5200, the resin supports filament winding with long pot life at processing temperatures and high glass-transition temperatures after the specified cure. Applications include aerospace, spacecraft, high-performance composite parts, and industrial composites. Final mechanical and thermal properties remain tied to the selected hardener, formulation, specimen, and cure schedule.

Key features

  • Low-viscosity processing profile: Typical viscosity is 3,000 to 6,000 cP at 50 deg C for reinforcement wet-out.
  • Long processing pot life: The MY 721/ARADUR 5200 system provides extended working time at processing temperatures.
  • High-temperature composite system: The specified formulation develops high glass-transition temperatures after cure.

Applications

Filament winding for aerospace, spacecraft, high-performance composite parts, and industrial composites in specified MY 721 systems.

Technical Specifications

General Properties
Appearance Appearance
clear brown liquid
Density (g) Density (g)
1.15-1.18 g/cm3
Mix Ratio Mix Ratio
100:35 by weight
Physical Properties
Viscosity Viscosity
3,000-6,000 mPa.s
Electrical Properties
Dielectric Strength Dielectric Strength
17.32 kV/mm
Surface Resistivity Surface Resistivity
7.4 x 10^16 Ohms/sq
Volume Resistivity Volume Resistivity
1.1 x 10^16 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical MY 721 resin-component data.

PropertyValueUnitMethod / condition
AppearanceClear brown liquid-As supplied
Density1.15 to 1.18g/cm^325 deg C
Viscosity3,000 to 6,000cP50 deg C
Epoxy equivalent weight111 to 117g/eqProduct value range